PC LEXAN™ 923A-116 SABIC INNOVATIVE NANSHA
207
Unit Price:$2699 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 116MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Material Certification
Technical Data Sheet
Material Description
- Material Properties:High rigidity|Weather resistance
- Application Areas:Communication equipment
- Color:--
- Grade:Injection grade
Material Certification

Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Specific Volume | ASTMD792 | 0.835 cm³/g | |
Melt Mass-Flow Rate | 300°C/1.2kg | ASTMD1238 | 15 g/10min |
Modeling Shrinkage | MD:3.20mm | 内部方法 | 0.50to0.70 % |
Moisture Absorption | 24hr | ASTMD570 | 0.15 % |
平衡,23°C | ASTMD570 | 0.35 % | |
平衡,100°C | ASTMD570 | 0.58 % | |
Outdoor Suitability | UL746C | f1 | |
Density / Specific Gravity | ASTMD792 | 1.21 g/cm³ | |
ASTMD792 | 1.22 g/cm³ | ||
Outdoor Suitability | UL746C | f1 |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Vicat Softening Temperature | ASTMD15255 | 152 °C | |
Linear thermal expansion coefficient | MD:-40到95°C | ASTME831 | 6.8E-05 cm/cm/°C |
Thermal Conductivity | ASTMC177 | 0.19 W/m/K | |
RTIElec | UL746 | 130 °C | |
Evolution Calendar intelligent importer | UL746 | 120 °C | |
RTIStr | UL746 | 130 °C | |
Heat Deflection Temperature | 0.45MPa,未退火,6.40mm | ASTMD648 | 138 °C |
1.8MPa,未退火,6.40mm | ASTMD648 | 132 °C | |
Thermal Conductivity | ASTMC177 | 0.19 W/m/K |
Optical | Test Condition | Test Method | Test Result |
---|---|---|---|
Index of Refraction | ASTMD542 | 1.586 | |
Transmittance | 2540µm | ASTMD1003 | 85.0 % |
Haze | 2540µm | ASTMD1003 | 1.0 % |
Index of Refraction | ASTMD542 | 1.586 |
Flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Rating | 1.5mm | UL94 | V-2 |
3.0mm | UL94 | V-0 |
Electrical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Dielectric Constant | 1MHz | ASTMD150 | 2.96 |
Dissipation Factor? | 50Hz | ASTMD150 | 9E-04 |
60Hz | ASTMD150 | 9E-04 | |
1MHz | ASTMD150 | 0.010 | |
Arc Resistance | ASTMD495 | PLC7 | |
Comparative Tracking Index | CTI | UL746 | PLC 3 |
High Amp Arc Ignition | HAI | UL746 | PLC 2 |
High Voltage Arc Tracking Rate | HVTR | UL746 | PLC 3 |
Hot-wire Ignition | HWI | UL746 | PLC 2 |
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm | |
Dielectric Strength | 3.20mm,inAir | ASTMD149 | 17 KV/mm |
Dielectric Constant | 50Hz | ASTMD150 | 3.01 |
60Hz | ASTMD150 | 3.01 | |
Arc Resistance | ASTMD495 | PLC7 | |
Volume Resistivity | ASTMD257 | >1.0E+17 ohms·cm |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Strength | 屈服 | ASTMD638 | 62.1 Mpa |
断裂 | ASTMD638 | 55.8 Mpa | |
Tensile Elongation | 屈服 | ASTMD638 | 7.0 % |
断裂 | ASTMD638 | 90 % | |
Flexural Modulus | 50.0mm跨距 | ASTMD790 | 2240 Mpa |
Flexural Strength | 屈服,50.0mm跨距 | ASTMD790 | 91.0 Mpa |
Taber Abrasion Resistance | 1000Cycles,1000g,CS-17转轮 | ASTMD1044 | 10.0 mg |
Hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Rockwell Hardness | M计秤 | ASTMD785 | 70 |
R计秤 | ASTMD785 | 118 |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Gardner Impact | 23°C | ASTMD3029 | 169 J |
Tensile Impact Strength | ASTMD1822 | 525 kJ/m² | |
ASTMD1822 | 525 kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.