Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Melt volume flow rate | 300°C/1.2kg | ISO1133 | 10.0 | cm3/10min |
Shrinkage rate | MD1 | 内部方法 | 0.50到0.70 | % |
Water absorption rate | Saturation,23°C | ISO62 | 0.35 | % |
Water absorption rate | Equilibrium,23°C,50%RH | ISO62 | 0.15 | % |
Outdoor applicability | | UL746C | f1 | |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Tensile modulus | | ISO527-2/1 | 2350 | Mpa |
Tensile stress | Yield | ISO527-2/50 | 63.0 | Mpa |
Tensile stress | Break | ISO527-2/50 | 65.0 | Mpa |
Tensile strain | Yield | ISO527-2/50 | 6.0 | % |
Tensile strain | Break | ISO527-2/50 | 100 | % |
Bending modulus 2 | | ISO178 | 2300 | Mpa |
Bending stress 3 | | ISO178 | 90.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
BallPressure Test | 125°C | IEC60695-10-2 | Pass | |
Linear coefficient of thermal expansion | MD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C |
thermal conductivity | | ISO8302 | 0.20 | W/m/K |
RTIElec | | UL746 | 130 | °C |
Evolution Calendar intelligent importer | | UL746 | 120 | °C |
RTI | | UL746 | 125 | °C |
0.45MPa, unannealed, 100mm span | | ISO75-2/Be | 136 | °C |
1.8MPa, unannealed, 100mm span | | ISO75-2/Ae | 125 | °C |
-- | | ISO306/B50 | 141 | °C |
-- | | ISO306/B120 | 142 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Relative permittivity | 50Hz | IEC60250 | 2.70 | |
Relative permittivity | 60Hz | IEC60250 | 2.70 | |
Relative permittivity | 1MHz | IEC60250 | 2.70 | |
Dissipation factor | 50Hz | IEC60250 | 1E-03 | |
Dissipation factor | 60Hz | IEC60250 | 1E-03 | |
Dissipation factor | 1MHz | IEC60250 | 0.010 | |
Leakage Trace Index | | IEC60112 | 225 | V |
Surface resistivity | | IEC60093 | >1.0E+15 | ohms |
Volume resistivity | | IEC60093 | >1.0E+15 | ohms·cm |
Dielectric strength | 3.20mm,in Oil | IEC60243-1 | 17 | KV/mm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Impact strength of simply supported beam gap 4 | -30°C | ISO179/1eA | 14 | kJ/m² |
Impact strength of simply supported beam gap 4 | 23°C | ISO179/1eA | 73 | kJ/m² |
Simply supported beam without notch impact strength 5 | -30°C | ISO179/1eU | 无断裂 | |
Simply supported beam without notch impact strength 5 | 23°C | ISO179/1eU | 无断裂 | |
Suspended wall beam notch impact strength 6 | -30°C | ISO180/1A | 12 | kJ/m² |
Suspended wall beam notch impact strength 6 | 23°C | ISO180/1A | 70 | kJ/m² |
Unscented Izod Impact Strength 7 | -30°C | ISO180/1U | 无断裂 | |
Unscented Izod Impact Strength 7 | 23°C | ISO180/1U | 无断裂 | |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Ball pressure hardness | H358/30 | ISO2039-1 | 95.0 | Mpa |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Refractive index | | ISO489 | 1.586 | |
transmissivity | 2540µm | ASTMD1003 | 88.0 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.50mm | UL94 | V-2 | |
UL flame retardant rating | 3.00mm | UL94 | V-0 | |
Burning wire flammability index | 1.00mm | IEC60695-2-12 | 960 | °C |
Hot filament ignition temperature | 1.00mm | IEC60695-2-13 | 850 | °C |
Extreme Oxygen Index | | ISO4589-2 | 35 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.