Need Help? Contact Us service@plas.com
Get App

POM TENAC™ MG210 ASAHI JAPAN

115
  • Unit Price:
    $5555 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:high viscosity High toughness Fatigue resistance Creep resistance High impact resistance high strength High rigidity Dimensional stability
  • Application Areas:Gear Conveyor accessories Engineering accessories Fasteners Automotive sector Shell bearing Gear Conveyor accessories Engineering accessories Fasteners Application in the automo Shell bearing
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Melt mass flow rate190°C/2.16kgISO11331.7g/10min
Shrinkage rateMD内部方法1.8到2.2%
Water absorption rate23°C,24hr,50%RHASTMD5700.20%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulusISO527-23150Mpa
Tensile stressYieldISO527-275.0Mpa
Tensile stress--ASTMD63879.0Mpa
elongationBreakASTMD638,ISO527-240%
Bending modulus--ASTMD7903040Mpa
Bending modulus--ISO1782900Mpa
bending strength ASTMD790108Mpa
Taber abraser ASTMD104413.0mg
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature0.45MPa,UnannealedASTMD648172°C
Hot deformation temperature0.45MPa,UnannealedISO75-2/B167°C
Hot deformation temperature1.8MPa,UnannealedASTMD648136°C
Hot deformation temperature1.8MPa,UnannealedISO75-2/A103°C
Linear coefficient of thermal expansionMDASTMD696,ISO11359-21E-04cm/cm/°C
specific heat1470J/kg/°C
thermal conductivity0.23W/m/K
Electrical performanceTest ConditionTest MethodTest ResultUnit
Surface resistivityASTMD2571.0E+16到1.0E+17ohms
Volume resistivity23°CASTMD2571.0E+15到1.0E+16ohms·cm
Dielectric strengthASTMD14918KV/mm
Dielectric constant23°C,1MHzASTMD1503.80
Dissipation factor23°C,1MHzASTMD1507E-03
Arc resistanceASTMD495250sec
hardnessTest ConditionTest MethodTest ResultUnit
Rockwell hardnessM-ScaleASTMD78594
Rockwell hardnessR-ScaleASTMD785120
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.