POM Delrin® 100T DUPONT USA
170
- Unit Price:
- $7720 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High rigidity High hardness Thermal stability high viscosity heat-resisting
- Application Areas:Thin walled products Electrical tools
- Color:--
- Grade:Toughened grade
Technical Data Sheet
Physical properties | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | ASTM D792/ISO 1183 | 1.37 |
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy impact strength | -30℃ | ISO-179/1eU | NB | NB |
Melt index | 190℃,2160g | ISO-1133 | 2 | g/10min |
Bending modulus | ISO-178 | 1.8 | GPa | |
Low temperature impact strength of simply supported beam | -30℃ | ISO-179/1eA | NB | NB |
Water absorption | ISO-62 | 0.9 | % | |
tensile strength | ISO-527-1,2 | 52 | Mpa | |
tensile elongation | ISO-75-1,2 | 75 | % | |
Charpy impact strength | 有Notched | ISO-179/1eA | 2.5 | J/cm |
Tensile modulus of elasticity | ISO-527-1,2 | 1.9 | GPa | |
Flexural elongation | ISO-527-1,2 | 26 | % | |
Impact resistance | ISO-180/1A | 20 | KJ/m | |
tensile elongation | nominal | ISO-527-1,2 | 50 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature (1.8MPa) | Annealed | ISO-75-1,2 | 85 | °C |
Melting point | ISO-3146C | 178 | °C | |
Hot deformation temperature | 0.46MPa | ISO-75-1,2 | 160 | °C |
1.8MPa | ISO-75-1,2 | 80 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Resistance to conductive tracks | 1mm | IEC-60112 | 600 | V |
Dielectric loss factor | 1MHz | IEC-60250 | 0.009 | |
Dielectric constant | 1MHz,1mm | IEC-60250 | 3.1 |
Processing performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
drying temperature | 80 | °C | ||
Melting point temperature | 200-210 | °C | ||
drying time | 2-4 | hour | ||
Moisture content | Max0.05 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.