ABS Terluran® HI-12 INEOS STYRO KOREA
183
- Unit Price:
- $3444 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility
- Application Areas:Helmet Electrical/Electronic App Electrical appliances Electronic field Household goods
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ISO1183 | 1.02 | g/cm³ | |
Melt volume flow rate | 220°C/10.0kg | ISO1133 | 14.0 | cm3/10min |
Shrinkage rate | ISO294-4 | 0.40到0.70 | % | |
Water absorption rate | Saturation,23°C | ISO62 | 1.0 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.21 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2 | 1900 | Mpa | |
Tensile stress | Yield,23°C | ISO527-2 | 40.0 | Mpa |
Tensile strain | Yield,23°C | ISO527-2 | 2.7 | % |
Bending stress | ISO178 | 58.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vicat softening temperature | -- | ISO306/A50 | 104 | °C |
-- | ISO306/B50 | 96.0 | °C | |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 8.0E-5到1.1E-4 | cm/cm/°C |
thermal conductivity | DIN52612 | 0.17 | W/m/K | |
Maximum operating temperature | 80 | °C | ||
Hot deformation temperature 3 | 0.45MPa,Annealed | ISO75-2/B | 102 | °C |
1.8MPa,Annealed | ISO75-2/A | 97.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Leakage Trace Index | IEC60112 | 600 | V | |
Volume resistivity | IEC60093 | 1E+15 | ohms·cm | |
Dielectric constant | 100Hz | IEC60250 | 2.90 | |
1.00mm,1MHz | 2.80 | |||
Dissipation factor | 100Hz | IEC60250 | 5.4E-03 | |
1MHz | IEC60250 | 8.2E-03 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Charpy Notched Impact Strength | -30°C | ISO179 | 11 | kJ/m² |
23°C | ISO179 | 30 | kJ/m² | |
Impact strength of simply supported beam without notch | -30°C | ISO179 | 160 | kJ/m² |
23°C | ISO179 | 无断裂 | ||
Impact strength of cantilever beam gap | 23°C | ASTMD256 | 35.0 | kJ/m² |
-30°C | ISO180/A | 11 | kJ/m² | |
23°C | ISO180/A | 31 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Sale | ISO2039-2 | 101 | |
Ball pressure hardness | ISO2039-1 | 80.0 | Mpa |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.6mm | UL94 | HB | |
3.2mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.