ABS TAITALAC® 5000 TAIDA TAIWAN
217
Unit Price:$1592 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 39MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High rigidity
- Application Areas:Electrical appliances Household goods Audiotape Shell
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ASTMD792 | 1.04 | g/cm³ | |
Melt mass flow rate | 200°C/5.0kg | ASTMD1238 | 2.0 | g/10min |
220°C/10.0kg | ASTMD1238 | 20 | g/10min | |
Shrinkage rate | MD | ASTMD955 | <0.40 | % |
Water absorption rate | 24hr | ASTMD570 | <0.30 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength 2 | Yield,23°C,3.18mm | ASTMD638 | 42.1 | Mpa |
Tensile strength 2 | Break,23°C,3.18mm | ASTMD638 | 35.2 | Mpa |
Elongation rate 2 | Break,23°C,3.18mm | ASTMD638 | 30 | % |
Bending modulus 3 | 23°C | ASTMD790 | 2550 | Mpa |
Bending strength 4 | Yield,23°C | ASTMD790 | 73.5 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,12.7mm | ASTMD648 | 83.0 | °C |
Vicat softening temperature | ASTMD15254 | 103 | °C | |
RTIElec | 1.6mm | UL746 | 60.0 | °C |
Evolution Calendar intelligent importer | 1.6mm | UL746 | 60.0 | °C |
RTIStr | 1.6mm | UL746 | 60.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
High arc combustion index | 1.57mm | UL746 | 200 | |
High voltage arc ignition resistance index | 1.57mm | UL746 | 0.00 | mm/min |
Hot-wireIgnition | 1.57mm | UL746 | 18 | sec |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of cantilever beam gap | 23°C,3.18mm | ASTMD256 | 200 | J/m |
23°C,6.35mm | ASTMD256 | 180 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Sale,23°C | ASTMD785 | 115 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FlameRating | 1.6mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.