TPV SARLINK® 4775B40 TEKNOR APEX BELGIUM
19
Unit Price:$2825 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Weather resistant grade
Technical Data Sheet
ageing | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Change rate of tensile strength in air - transverse flow rate | 135°C,1000hr | ASTMD573 | -12 | % |
100%Strain,135°C,1000hr | ASTMD573 | 5.0 | % | |
150°C,168hr | ASTMD573 | -22 | % | |
100%Strain,150°C,168hr | ASTMD573 | 2.0 | % | |
135°C,1000hr | ISO188 | -12 | % | |
100%Strain135°C,1000hr | ISO188 | 5.0 | % | |
150°C,168hr | ISO188 | -22 | % | |
100%Strain150°C,168hr | ISO188 | 2.0 | % | |
Change rate of ultimate elongation in air - lateral flow rate | 135°C,1000hr | ASTMD573 | -16 | % |
150°C,168hr | ASTMD573 | -29 | % | |
Tensile stress variation during fracture in air - transverse flow rate | 135°C,1000hr | ISO188 | -16 | % |
150°C,168hr | ISO188 | -29 | % | |
The rate of change in hardness of an air hardness tester | Shore A,135°C,1000hr | ASTMD573 | 3.0 | |
Shore A,150°C,168hr | ASTMD573 | 1.0 | ||
Change rate of Shore hardness in air | Shore A,135°C,1000hr | ISO188 | 3.0 | |
Shore A,150°C,168hr | ISO188 | 1.0 | ||
Volume change | 125°C,70hr,在IRM903油中 | ASTMD471 | 74 | % |
125°C,70hr,在IRM903油中 | ISO1817 | 74 | % |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tear strength - transverse flow rate | ASTMD624 | 33.3 | kN/m | |
Tear strength - transverse flow rate 2 | ISO34-1 | 33 | kN/m | |
Permanent compression deformation | 23°C,22hr | ASTMD395 | 24 | % |
70°C,22hr | ASTMD395 | 36 | % | |
125°C,70hr | ASTMD395 | 52 | % | |
23°C,22hr | ISO815 | 24 | % | |
70°C,22hr | ISO815 | 36 | % | |
125°C,70hr | ISO815 | 52 | % | |
Tensile stress | Across Flow:100%Strain | ISO37 | 3.10 | Mpa |
流量:100%Strain | ISO37 | 3.50 | Mpa | |
Tensile strength | Break | ASTMD412 | 6.60 | Mpa |
流量:Break | ASTMD412 | 6.00 | Mpa | |
Tensile stress | Break | ISO37 | 6.60 | Mpa |
流量:Break | ISO37 | 6.00 | Mpa | |
elongation | Break | ASTMD412 | 490 | % |
流量:Break | ASTMD412 | 410 | % | |
Break | ISO37 | 490 | % | |
流量:Break | ISO37 | 410 | % | |
Tensile stress | Across Flow:100%Strain | ASTMD412 | 3.10 | Mpa |
流量:100%Strain | ASTMD412 | 3.50 | Mpa |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,5sec,挤塑 | ISO868 | 74 | |
Shore A,5sec,Injection | ISO868 | 76 | ||
Shore A,5sec,挤塑 | ASTMD2240 | 74 | ||
Shore A,5sec,Injection | ASTMD2240 | 76 |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
ApparentShearViscosity-Capillary@206/s | 200°C | ISO11443 | 220 | Pa·s |
200°C | ASTMD3835 | 220 | Pa·s |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.
Contact Us
Get App
Top