Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Density/specific gravity | | ASTMD792,ISO1183 | 1.20 | g/cm³ |
Melt mass flow rate | 300°C/1.2kg | ASTMD1238 | 22 | g/10min |
Melt volume flow rate | 300°C/1.2kg | ISO1133 | 21.0 | cm3/10min |
Shrinkage rate | MD:--1 | 内部方法 | 0.50到0.70 | % |
Shrinkage rate | MD:3.20mm | 内部方法 | 0.50到0.70 | % |
Saturation, 23 ° C | | ISO62 | 0.35 | % |
Balance, 23 ° C | | ASTMD570 | 0.35 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
-- | | ISO527-2/1 | 2350 | Mpa |
Surrender 3 | | ASTMD638 | 63.0 | Mpa |
yield | | ISO527-2/50 | 63.0 | Mpa |
Surrender 4 | | ASTMD638 | 6.0 | % |
yield | | ISO527-2/50 | 6.0 | % |
Fracture 5 | | ASTMD638 | >70 | % |
crack | | ISO527-2/50 | >70 | % |
50.0mm span 6 | | ASTMD790 | 2300 | Mpa |
--7 | | ISO178 | 2300 | Mpa |
--8 | | ISO178 | 90.0 | Mpa |
--2 | | ASTMD638 | 2350 | Mpa |
Yield, 50.0mm span 9 | | ASTMD790 | 90.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
1.8MPa, unannealed, 64.0mm span 14 | | ISO75-2/Af | 122 | °C |
Vicat softening temperature | | ISO306/B50,ASTMD152515 | 140 | °C |
BallPressure Test | 125°C | IEC60695-10-2 | Pass | |
-40 to 95 ° C | | ASTME831 | 7E-05 | cm/cm/°C |
23 to 80 ° C | | ISO11359-2 | 7E-05 | cm/cm/°C |
thermal conductivity | | ASTMC177,ISO8302 | 0.20 | W/m/K |
0.45MPa, unannealed, 3.20mm | | ASTMD648 | 133 | °C |
0.45MPa, unannealed, 64.0mm span 13 | | ISO75-2/Bf | 133 | °C |
1.8MPa, unannealed, 3.20mm | | ASTMD648 | 122 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Dissipation factor | 60Hz | ASTMD150,IEC60250 | 1E-03 | |
Dissipation factor | 1MHz | ASTMD150,IEC60250 | 0.010 | |
Volume resistivity | | ASTMD257,IEC60093 | >1.0E+15 | ohms·cm |
Dielectric strength | 1.60mm | ASTMD149,IEC60243-1 | 27 | KV/mm |
Dielectric constant | 60Hz | ASTMD150,IEC60250 | 3.00 | |
Dielectric constant | 1MHz | ASTMD150,IEC60250 | 3.00 | |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
23°C | | ASTMD256 | 640 | J/m |
-30°C10 | | ISO180/1A | 12 | kJ/m² |
23°C11 | | ISO180/1A | 65 | kJ/m² |
23°C | | ASTMD4812,ISO180/1U | 无断裂 | |
-30°C12 | | ISO180/1U | 无断裂 | |
Dart impact equipped with measuring instruments | 23°C,EnergyatPeakLoad | ASTMD3763 | 55.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
R-grade | | ASTMD785 | 120 | |
R scale | | ISO2039-2 | 120 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Refractive index | | ASTMD542,ISO489 | 1.586 | |
transmissivity | 2540µm | ASTMD1003 | 88.0到90.0 | % |
Haze | 2540µm | ASTMD1003 | <0.80 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 1.60mm | UL94 | V-2 | |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.