PP ExxonMobil™ PP7033E3 EXXONMOBIL USA
129
- Unit Price:
- $1528 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Block copolymer High mobility High rigidity High impact resistance
- Application Areas:Industrial containers Industrial applications container Plastic barrel Plastic box Barrel Shell Toy Consumer product applicat Rigid package Loading box
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 230°C/2.16kg | ASTMD1238 | 8.0 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2/1 | 1290 | Mpa | |
Tensile strength | Yield3 | ASTMD638 | 23.9 | Mpa |
Yield | ISO527-2/50 | 23.1 | Mpa | |
elongation | Yield3 | ASTMD638 | 6.5 | % |
Yield | ISO527-2/50 | 5.6 | % | |
Bending modulus | 1%Secant4 | ASTMD790A | 1140 | Mpa |
1%Secant5 | ASTMD790B | 1280 | Mpa | |
--6 | ISO178 | 1190 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/Bf | 85.3 | °C |
0.45MPa,Annealed | ASTMD648 | 114 | °C | |
1.8MPa,Unannealed | ISO75-2/A | 50.9 | °C | |
0.45MPa,Unannealed | ASTMD648 | 90.2 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of cantilever beam gap | -18°C | ISO180/1A | 5.7 | kJ/m² |
23°C | ISO180/1A | 13 | kJ/m² | |
Falling hammer impact 7 | -29°C,3.18mm | ASTMD5420 | 28.1 | J |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 4.3 | kJ/m² |
-20°C | ISO179/1eA | 5.4 | kJ/m² | |
0°C | ISO179/1eA | 6.7 | kJ/m² | |
23°C | ISO179/1eA | 14 | kJ/m² | |
Impact strength of cantilever beam gap | 23°C | ASTMD256A | 280 | J/m |
-40°C | ISO180/1A | 4.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | ASTMD785 | 89 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.