Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Water absorption rate | 23°C,24hr | ASTMD570 | 0.40 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Fatigue-%ofstresstofailure5 | | ASTMD638 | 35 | % |
bending strength | | ASTMD790 | 221 | Mpa |
Compressive modulus | | ASTMD695 | 5860 | Mpa |
compressive strength | --2 | ASTMD695 | 393 | Mpa |
compressive strength | 10%Strain | ASTMD695 | 345 | Mpa |
friction coefficient | Steel - Dynamic | | 0.16 | |
friction coefficient | Steel - Static | | 0.15 | |
friction coefficient | 与金属-动态3 | | 0.16 | |
friction coefficient | 与金属-动态4 | | 0.18 | |
friction coefficient | 与金属-静态3 | | 0.14 | |
friction coefficient | 与金属-静态4 | | 0.16 | |
Tensile modulus | | ASTMD638 | 5860 | Mpa |
Tensile strength | | ASTMD638 | 159 | Mpa |
elongation | Break | ASTMD638 | 3.0 | % |
Bending modulus | | ASTMD790 | 6550 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 1.8MPa,Unannealed | ASTMD648 | 435 | °C |
Glass transition temperature | | DMA | 427 | °C |
Linear coefficient of thermal expansion | MD:24to149°C | TMA | 2.3E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | MD:199to299°C | TMA | 3.2E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | MD:导热系数(25°C) | TMA | 0.40 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | | ASTMD257 | 2E+15 | ohms·cm |
Dielectric strength | | ASTMD149 | 23 | KV/mm |
Dielectric constant | 1kHz | ASTMD150 | 3.40 | |
Dielectric constant | 10kHz | ASTMD150 | 3.40 | |
Dielectric constant | 100kHz | ASTMD150 | 3.30 | |
Dissipation factor | 1kHz | ASTMD150 | 0.0 | |
Dissipation factor | 10kHz | ASTMD150 | 3E-03 | |
Dissipation factor | 100kHz | ASTMD150 | 0.034 | |
Arc resistance | | ASTMD495 | 185 | sec |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Cantilever beam without notch impact strength | | ASTMD256 | 590 | J/m |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | E-Sale | ASTMD785 | 104 | |
Rockwell hardness | M-Scale | ASTMD785 | >125 | |
Shore hardness | Shore D | ASTMD2240 | 95 | |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
Extreme Oxygen Index | | ASTMD2863 | 58 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.