PPA/F/PTFE LNP™ LUBRICOMP™ UFL-4036 SABIC INNOVATIVE US
136
- Unit Price:
- $4857 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 61.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability Flame retardant
- Application Areas:tubing Lighting applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:24hr | ASTMD955 | 0.20to0.40 | % |
TD:24hr | ASTMD955 | 0.80to1.0 | % | |
Water absorption rate | 24hr,50%RH | ASTMD570 | 0.15 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.25 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | --2 | ASTMD638 | 15400 | Mpa |
--3 | ASTMD638 | 15400 | Mpa | |
ISO527-2/1 | 12600 | Mpa | ||
Tensile strength 4 | Yield | ASTMD638 | 189 | Mpa |
FlexuralStrength5 | Break,50.0mmSpan | ASTMD790 | 233 | Mpa |
friction coefficient | Dynamic | ASTMD3702Modified | 0.48 | |
Static | ASTMD3702Modified | 0.52 | ||
Wear factor | Ring | ASTMD3702Modified | 0.100 | 10^-10in^5-min/ft-lb-hr |
Washer | ASTMD3702Modified | 5.00 | 10^-10in^5-min/ft-lb-hr | |
Tensile stress | Yield | ISO527-2/5 | 192 | Mpa |
Tensile strength 4 | Break | ASTMD638 | 189 | Mpa |
Tensile stress | Break | ISO527-2/5 | 192 | Mpa |
Elongation rate 4 | Yield | ASTMD638 | 1.8 | % |
Tensile strain | Yield | ISO527-2/5 | 2.0 | % |
Elongation rate 4 | Break | ASTMD638 | 1.7 | % |
Tensile strain | Break | ISO527-2/5 | 2.0 | % |
Bending modulus 5 | 50.0mmSpan | ASTMD790 | 10600 | Mpa |
Bending modulus 6 | ISO178 | 11300 | Mpa | |
FlexuralStrength5 | Yield,50.0mmSpan | ASTMD790 | 242 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTMD648 | 277 | °C |
Hot deformation temperature 8 | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 273 | °C |
Linear coefficient of thermal expansion | MD:-30to30°C | ASTMD696 | 2.1E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 4.5E-05 | cm/cm/°C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Multi axis Instrumented Impact Energy | ISO6603-2 | 2.00 | J | |
NotchedIzodImpactStrength7 | 23°C | ISO180/1A | 9.1 | kJ/m² |
UnnotchedIzodImpactStrength7 | 23°C | ISO180/1U | 47 | kJ/m² |
Dart impact equipped with measuring instruments | 23°C,TotalEnergy | ASTMD3763 | 8.90 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.