PA66/C/PTFE LNP™ LUBRICOMP™ RCL-4036 BK8115 SABIC INNOVATIVE US
122
- Unit Price:
- $5716 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 36MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Low temperature impact re Thermal stability
- Application Areas:Electronic and Electrical Automotive components
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:24hr | ASTMD955 | 0.10 | % |
TD:24hr | ASTMD955 | 0.70 | % | |
TD:24hr | ISO294-4 | 0.72 | % | |
MD:24hr | ISO294-4 | 0.11 | % | |
Water absorption rate | 24hr,50%RH | ASTMD570 | 0.53 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.84 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress | Break | ISO527-2 | 245 | Mpa |
Tensile strain | Break | ISO527-2 | 1.8 | % |
Bending stress | ISO178 | 396 | Mpa | |
friction coefficient | Dynamic | ASTMD3702Modified | 0.36 | |
Static | ASTMD3702Modified | 0.30 | ||
Tensile modulus | ISO527-2/1 | 22600 | Mpa | |
elongation | Break | ASTMD638 | 0.90 | % |
Bending modulus | ASTMD790 | 18400 | Mpa | |
ISO178 | 22700 | Mpa | ||
bending strength | ASTMD790 | 373 | Mpa | |
Tensile modulus 2 | ASTMD638 | 32400 | Mpa | |
Tensile strength | Break | ASTMD638 | 182 | Mpa |
Wear factor - Washer | ASTMD3702Modified | 15.0 | 10^-10in^5-min/ft-lb-hr |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature 4 | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | >240 | °C |
Hot deformation temperature | 1.8MPa,Unannealed,3.20mm | ASTMD648 | 255 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Suspended wall beam gap impact strength 3 | 23°C | ISO180/1A | 11 | kJ/m² |
UnnotchedIzodImpactStrength3 | 23°C | ISO180/1U | 69 | kJ/m² |
Dart impact equipped with measuring instruments | 23°C,EnergyatPeakLoad | ASTMD3763 | 10.2 | J |
Multi axis Instrumented Impact Energy | ISO6603-2 | 3.91 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.