Need Help? Contact Us service@plas.com
Get App

PA66/PTFE LNP™ LUBRICOMP™  RBL-4036 SABIC INNOVATIVE US

207
  • Unit Price:
    $5455 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    40MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Low extract Wear resistance Corrosion resistance
  • Application Areas:Gear cover Lampholder cover building materials
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9552.0到4.0%
Shrinkage rateTD:24hrASTMD9551.0到3.0%
Water absorption rate24hr,50%RHASTMD5700.41%
Water absorption rateEquilibrium,23°C,50%RHISO620.58%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus--2ASTMD6383990Mpa
Tensile modulus--ISO527-2/13930Mpa
Tensile strengthBreak3ASTMD63864.0Mpa
friction coefficientDynamicASTMD3702Modified0.47
friction coefficientStaticASTMD3702Modified0.44
Wear factorRingASTMD3702Modified8.0010^-10in^5-min/ft-lb-hr
Wear factorWasherASTMD3702Modified41.010^-10in^5-min/ft-lb-hr
Tensile strengthBreakISO527-2/564.0Mpa
elongationYield3ASTMD6388.5%
elongationBreak3ASTMD63810%
elongationBreakISO527-2/58.3%
Bending modulus50.0mmSpan4ASTMD7903740Mpa
Bending modulus--5ISO1783570Mpa
Bending stressISO178107Mpa
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTMD648236°C
Hot deformation temperature0.45MPa,Unannealed,64.0mmSpan7ISO75-2/Bf203°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD64883.0°C
Hot deformation temperature1.8MPa,Unannealed,64.0mmSpan7ISO75-2/Af73.0°C
Linear coefficient of thermal expansionMD:-30to30°CASTMD6968.3E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTMD6966.9E-05cm/cm/°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Cantilever beam without notch impact strength23°CASTMD4812440J/m
Cantilever beam without notch impact strength23°C6ISO180/1U27kJ/m²
Dart impact equipped with measuring instruments23°C,TotalEnergyASTMD37635.60J
Dart impact equipped with measuring instruments--ISO6603-21.34J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.