UHMWPE GUR® GHR 8110 CELANESE USA
223
- Unit Price:
- $2985 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 119.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:wear resistant High impact resistance
- Application Areas:Automotive Applications transportation industry
- Color:--
- Grade:Wear resistant grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 190°C/21.6kg | ASTMD1238 | 1.4 | g/10min |
190°C/2.16kg | ISO1133 | 1.3 | g/10min | |
Stickiness number | ISO307 | 600 | cm³/g | |
Intrinsic viscosity | ISO1628-3 | 6.0 | dl/g |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strain | Yield | ISO527-2/1A/50 | 9.0 | % |
Nominal tensile fracture strain | ISO527-2/1A/50 | >50 | % | |
Tensile creep modulus | 1hr | ISO899-1 | 680 | Mpa |
1000hr | ISO899-1 | 340 | Mpa | |
WearbySandslurryMethod3 | 内部方法 | 310 | ||
Wear amount | 内部方法 | 250 | ||
Tensile modulus | ISO527-2/1A/1 | 1100 | Mpa | |
Tensile stress | Yield | ISO527-2/1A/50 | 26.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear coefficient of thermal expansion | MD | ASTMD696,ISO11359-2 | 2E-04 | cm/cm/°C |
specific heat | 23°C | 内部方法 | 1840 | J/kg/°C |
thermal conductivity | 23°C | 内部方法 | 0.41 | W/m/K |
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 75.0 | °C |
1.8MPa,Unannealed | ISO75-2/A | 41.0 | °C | |
Vicat softening temperature | ASTMD1525,ISO306/B50 | 80.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | -- | ASTMD257 | >1.0E+13 | ohms |
-- | IEC60093 | >1.0E+12 | ohms | |
Volume resistivity | -- | ASTMD257 | >1.0E+15 | ohms·cm |
-- | IEC60093 | >1.0E+14 | ohms·cm | |
Dielectric strength | IEC60243-1 | 40 | KV/mm | |
Dielectric constant | 1MHz | ASTMD150 | 2.90 | |
100Hz | IEC60250 | 2.00 | ||
1MHz | IEC60250 | 2.00 | ||
Dissipation factor | 100Hz | IEC60250 | 2E-04 | |
1MHz | IEC60250 | 4E-04 | ||
Leakage Trace Index | IEC60112 | 600 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
CharpyImpactStrength4 | ISO1152-2 | 25.0 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore D | ASTMD2240 | 63 | |
Shore D,15sec | ISO868 | 63 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.6mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.