Need Help? Contact Us service@plas.com
Get App

PC/PET Makroblend®  UT250 COVESTRO GERMANY

195
  • Unit Price:
    $4117 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    17MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High mobility Dimensional stability High temperature resistan
  • Application Areas:Electrical field Electronic field
  • Color:--
  • Grade:Flame retardant grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Melt volume flow rate265°C/5.0kgISO113322.0cm3/10min
Shrinkage rateTD2ISO25770.60to0.80%
Shrinkage rateTD:90°C,1hrISO25770.10to0.20%
Shrinkage rateMD2ISO25770.60to0.80%
Shrinkage rateMD:90°C,1hrISO25770.10to0.20%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus23°CISO527-2/12250Mpa
Tensile stressYield,23°CISO527-2/5055.0Mpa
Tensile stressBreak,23°CISO527-2/5050.0Mpa
Tensile strainYield,23°CISO527-2/505.0%
Nominal tensile fracture strain23°CISO527-2/50>50%
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature0.45MPa,UnannealedISO75-2/B125°C
Hot deformation temperature1.8MPa,UnannealedISO75-2/A110°C
Vicat softening temperatureISO306/B120140°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Impact strength of cantilever beam gap-30°CISO180/1CNoBreak
Impact strength of cantilever beam gap-20°CISO180/A40kJ/m²
Impact strength of cantilever beam gap23°CISO180/A50kJ/m²
Impact strength of cantilever beam gap23°CISO180/1CNoBreak
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.