PFA HYFLON® PFA P420 SOLVAY USA
126
- Unit Price:
- $26122 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 372°C/5.0kg | ASTMD1238 | 1.5到3.0 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus 2 | 23°C | ASTMD1708 | 500到600 | Mpa |
Tensile strength | Break,23°C | ASTMD1708 | >26.0 | Mpa |
elongation | Break,23°C | ASTMD1708 | >300 | % |
Bending life | 300.0µm | ASTMD2176 | 9.0E+4到1.2E+5 | cycles |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Continuous use temperature | 260 | °C | ||
Melting temperature | ASTMD3307 | 300到310 | °C | |
Crystallization peak temperature | DSC | DSC | 275到285 | °C |
Linear coefficient of thermal expansion | MD | ASTMD696 | 1.2E-4到2.0E-4 | cm/cm/°C |
specific heat | 23°C | DSC | 900到1100 | J/kg/°C |
thermal conductivity | 40°C | ASTMC177 | 0.20 | W/m/K |
Crystallization heat | DSC | 25.0到35.0 | J/g | |
Fusion heat | DSC | 25.0到35.0 | J/g |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTMD257 | >1.0E+17 | ohms | |
Volume resistivity | ASTMD257 | >1.0E+17 | ohms·cm | |
Dielectric strength | ASTMD149 | 35到40 | KV/mm | |
Dielectric constant | 23°C,50Hz | ASTMD150 | 2.10 | |
23°C,100kHz | ASTMD150 | 2.10 | ||
Dissipation factor | 23°C,50Hz | ASTMD150 | <5.0E-4 | |
23°C,100kHz | ASTMD150 | <5.0E-4 |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore D | ASTMD2240 | 59 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | UL94 | V-0 | ||
Extreme Oxygen Index | ASTMD2863 | 95 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.