PC/PBT XENOY™ 6240-NC SABIC INNOVATIVE US
157
Unit Price:$3612 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 33MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced Low warpage
- Application Areas:Automotive Applications Casters Plastic bag
- Color:--
- Grade:Injection grade
Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
收缩率 | MD | 内部方法 | 0.33 | % |
MD:3.20mm | 内部方法 | 0.30到0.40 | % | |
TD | 内部方法 | 0.38 | % | |
吸水率 | 饱和,23°C | ISO62 | 0.10 | % |
平衡,23°C,50%RH | ISO62 | 0.030 | % | |
熔体体积流动速率 | 260°C/2.16kg | ISO1133 | 15.0 | cm3/10min |
熔体质量流动速率 | 260°C/2.16kg | ASTMD1238 | 17 | g/10min |
机械性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
23°C | ASTMD256 | 86 | J/m | |
装有测量仪表的落镖冲击 | -30°C,TotalEnergy | ASTMD3763 | 35.0 | J |
23°C,TotalEnergy | ASTMD3763 | 56.0 | J | |
简支梁缺口冲击强度 | 23°C | ISO179/1eA | 6.0 | kJ/m² |
-30°C | ASTMD256 | 60 | J/m | |
ISO180/1A | 7.0 | kJ/m² | ||
23°C | ISO180/1A | 7.0 | kJ/m² | |
屈服 | ISO527-2/5 | 56.0 | Mpa | |
ISO527-2/5 | 3.0 | % | ||
断裂 | ISO527-2/5 | 29.0 | Mpa | |
ISO527-2/5 | 25 | % | ||
屈服 | ASTMD638 | 55.0 | Mpa | |
断裂 | ASTMD638 | 40.0 | Mpa | |
50.0mm跨距 | ASTMD790 | 4400 | Mpa | |
-- | ISO178 | 4510 | Mpa | |
ISO178 | 101 | Mpa | ||
ASTMD638 | 4350 | Mpa | ||
屈服 | ASTMD638 | 3.0 | % | |
断裂 | ASTMD638 | 35 | % | |
屈服,50.0mm跨距 | ASTMD790 | 96.0 | Mpa |
热性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
-- | ISO 1183 | 97.0 | °C | |
ISO306/B120 | 100 | °C | ||
流动:-40到40°C | ASTME831 | 4.9E-05 | cm/cm/°C | |
ISO11359-2 | 4.8E-05 | cm/cm/°C | ||
横向:-40到40°C | ASTME831 | 6.4E-05 | cm/cm/°C | |
ISO11359-2 | 6.3E-05 | cm/cm/°C | ||
1.8MPa,未退火,64.0mm跨距 | ISO75-2/Af | 86.0 | °C | |
1.8MPa,未退火,6.40mm | ASTMD648 | 90.0 | °C |
可燃性 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL阻燃等级 | 0.800mm,TestingbySABIC | UL94 | V-0 | |
1.50mm,TestingbySABIC | UL94 | 5VB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.