PCTG Tritan™ FX200 EASTMAN USA
154
- Unit Price:
- $4046 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 71.8MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Chemical resistance Hydrolysis resistance
- Application Areas:Electrical applications Household daily necessiti
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | 23°C,24hr,0.254mm | ASTMD570 | 0.50 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tab | 23°C,250.0µm | ASTMD1044 | 20Haze | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
specific heat | 60°C | DSC | 1700 | J/kg/°C |
100°C | DSC | 1900 | J/kg/°C | |
150°C | DSC | 2300 | J/kg/°C | |
200°C | DSC | 2400 | J/kg/°C | |
250°C | DSC | 2600 | J/kg/°C | |
Melting temperature | 119 | °C | ||
Linear coefficient of thermal expansion | MD:23°C | ASTMD696 | 8E-05 | cm/cm/°C |
film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hammer impact 4 | -30°C,250µm | ASTMD1709A | 830 | g |
-18°C,250µm | ASTMD1709A | 830 | g | |
23°C,250µm | ASTMD1709A | 830 | g | |
Tear resistance of pants type 5 | MD:250µm | ISO6383-1 | 10.0 | N/mm |
TD:250µm | ISO6383-1 | 9.00 | N/mm | |
Oxygen permeability rate | 23°C,250µm,50%RH | ASTMD3985 | 44 | cm³·mm/m²/atm/24hr |
Water vapor permeability | 23°C,100%RH,250µm | ASTMF1249 | 4.0 | g/m²/24hr |
38°C,100%RH,250µm | ASTMF1249 | 10 | g/m²/24hr | |
CarbonDioxidePermeability | 23°C,254.0µm | ASTMD1434 | 210 | cm³·mm/m²/atm/24hr |
Elmondov tear strength | MD:23°C,250.0µm | ASTMD1922 | 4 | N |
Film thickness - tested | 250 | µm | ||
Membrane puncture strength 3 | 250µm | ASTMD3763 | 4.50 | J |
Secant modulus MD | 250µm | ASTMD882 | 1500 | Mpa |
Secant modulus TD | 250µm | ASTMD882 | 1400 | Mpa |
Tensile strength MD | Yield,250μm | ASTMD882 | 43.0 | Mpa |
Tensile strength TD | Yield,250µm | ASTMD882 | 41.0 | Mpa |
Tensile strength MD | Break,250µm | ASTMD882 | 57.0 | Mpa |
Tensile strength TD | Break,250µm | ASTMD882 | 42.0 | Mpa |
Tensile strain MD | Yield,250µm | ASTMD882 | 8.0 | % |
Tensile strain TD | Yield,250µm | ASTMD882 | 8.0 | % |
Elongation MD | Break,250μm | ASTMD882 | 110 | % |
Tensile strain TD | Break,250µm | ASTMD882 | 120 | % |
Elmondov tear strength | TD:23°C,250.0µm | ASTMD1922 | 4 | N |
PPTTearResistance | MD:23°C,250.0µm | 40 | N | |
TD:23°C,250.0µm | 40 | N | ||
Tear resistant ductility | MD:23°C,250.0µm | ASTMD1938 | 310 | gf |
TD:23°C,250.0µm | ASTMD1938 | 200 | gf |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
gloss | 60°,250µm | ASTMD2457 | 158 | |
Refractive index | ASTMD542 | 1.540 | ||
transmissivity | 250µm | ASTMD1003 | 93.0 | % |
Haze | 250µm | ASTMD1003 | 0.80 | % |
Huangdu Index | 250mm | ASTMD1925 | 0.50 | YI |
UVTransmittance8 | 250.0µm | 89 | % |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
SurfaceEnergy | Dispersive:23°C,250.0µm | ASTMD5946 | 39 | dyne/cm |
Polar:23°C,250.0µm | ASTMD5946 | 8 | dyne/cm | |
Total:23°C,250.0µm | ASTMD5946 | 47 | dyne/cm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.