TPV Santoprene™ 251-92 CELANESE USA
116
- Unit Price:
- $9431 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:heat-resisting Aging resistance Low temperature flexibili Flame retardant Dimensional stability Ozone resistant Recyclable Chemical resistance Fatigue resistance
- Application Areas:Cable Cable sheath Wire and cable applicatio Application in the automo Automotive Applications Flexible cable sheath
- Color:--
- Grade:Injection grade
Technical Data Sheet
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
RTIElec | UL746 | 90.0 | °C | |
RTIStr | 1.5mm | UL746 | 85.0 | °C |
3.0mm | UL746 | 90.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric strength | 23°C,2.00mm | ASTMD149 | 31 | KV/mm |
Compared to the anti leakage trace index | CTI | UL746 | PLC0 | |
High arc combustion index | HAI | UL746 | PLC0 | |
High voltage arc ignition resistance index | PLC | UL746 | PLC6 | |
High voltage arc tracing rate | HVTR | UL746 | PLC2 | |
Hot wire ignition | HWI | UL746 | PLC3 |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress transverse flow rate | 100%Strain,23°C | ASTMD412 | 7.20 | Mpa |
100%Strain,23°C | ISO37 | 7.20 | Mpa | |
Tensile strength - transverse flow rate | Break,23°C | ASTMD412 | 13.9 | Mpa |
Tensile strength TD | Break,23°C | ISO37 | 13.9 | Mpa |
Elongation rate - lateral flow rate | Break,23°C | ASTMD412 | 630 | % |
Break,23°C | ISO37 | 630 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,15sec,23°C | ISO868 | 98 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.5mm | UL94 | V-0 | |
3.0mm | UL94 | V-0 | ||
Extreme Oxygen Index | ASTMD2863 | 26 | % | |
ISO4589-2 | 26 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.