TPV Santoprene™ 701-80 CELANESE USA
105
- Unit Price:
- $5481 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Dimensional stability Ozone resistant Recyclable Low tenderness Oil resistant
- Application Areas:Industrial applications Application in the automo Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittle temperature | ASTMD746 | -32.0 | °C | |
ISO812 | -32.0 | °C |
ageing | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Change rate of tensile strength | 125°C,70hr,inIRM903Oil | ASTMD471 | -38 | % |
The rate of change in tensile strength in air | 125°C,168hr | ASTMD573 | 6.0 | % |
125°C,168hr | ISO188 | 6.0 | % | |
ChangeinUltimateElongationAir | 125°C,168hr | ASTMD573 | -37 | % |
ChangeinDurometerHardnessAir | ShoreA,125°C,168hr | ASTMD573 | 2.0 | |
ChangeinShoreHardnessinAir | ShoreA,125°C,168hr | ISO188 | 2.0 | |
ChangeinTensileStress | 125°C,70hr,inIRM903Oil | ISO1817 | -38 | % |
ChangeinUltimateElongation | 125°C,70hr,inIRM903Oil | ASTMD471 | -48 | % |
ChangeinTensileStrainatBreak | 125°C,70hr,inIRM903Oil | ISO1817 | -48 | % |
Volume change | 125°C,70hr,在IRM903油中 | ASTMD471 | 4.0 | % |
125°C,70hr,在IRM903油中 | ISO1817 | 4.0 | % |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tear strength - transverse flow rate 2 | 23°C | ASTMD624 | 30.0 | kN/m |
TearStrength-AcrossFlow3 | 23°C | ISO34-1 | 30 | kN/m |
CompressionSet4 | 70°C,22hr | ASTMD395B | 30 | % |
125°C,70hr | ASTMD395B | 47 | % | |
Compression permanent deformation 4 | 70°C,22hr | ISO815 | 30 | % |
125°C,70hr | ISO815 | 47 | % | |
Tensile stress transverse flow rate | 100%Strain,23°C | ASTMD412 | 5.20 | Mpa |
100%Strain,23°C | ISO37 | 5.20 | Mpa | |
Tensile strength - transverse flow rate | Break,23°C | ASTMD412 | 8.80 | Mpa |
Tensile strength TD | Break,23°C | ISO37 | 8.80 | Mpa |
Elongation rate - lateral flow rate | Break,23°C | ASTMD412 | 290 | % |
Break,23°C | ISO37 | 290 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,15sec,23°C | ISO868 | 83 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.