TPV Santoprene™ 8221-60 CELANESE USA
106
- Unit Price:
- $4234 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:Architectural application expansion joint Outdoor applications Glazing
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Outdoor applicability | UL746C | f1 |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittle temperature | ASTMD746 | -63.0 | °C | |
ISO812 | -63.0 | °C | ||
RTIElec | UL746 | 100 | °C | |
RTIStr | UL746 | 85.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric strength | 23°C,2.00mm | ASTMD149 | 31 | KV/mm |
DielectricConstant | 23°C,2.01mm | ASTMD150 | 2.30 | |
23°C,2.01mm | IEC60250 | 2.30 |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress transverse flow rate | 100%Strain,23°C | ASTMD412 | 2.20 | Mpa |
100%Strain,23°C | ISO37 | 2.20 | Mpa | |
Tensile strength - transverse flow rate | Break,23°C | ASTMD412 | 5.70 | Mpa |
Tensile strength TD | Break,23°C | ISO37 | 5.70 | Mpa |
Elongation rate - lateral flow rate | Break,23°C | ASTMD412 | 470 | % |
Break,23°C | ISO37 | 470 | % | |
Compression permanent deformation 2 | 70°C,22hr | ASTMD395B | 32 | % |
125°C,70hr | ASTMD395B | 60 | % | |
Compression permanent deformation 3 | 70°C,22hr | ISO815 | 32 | % |
125°C,70hr | ISO815 | 60 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,15sec,23°C | ISO868 | 64 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 1.1mm | UL94 | HB | |
3.0mm | UL94 | HB |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.