TPV Santoprene™ 121-85M100 CELANESE USA
102
- Unit Price:
- $6098 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:dimensional stability UV resistance Recyclable materials Good forming performance High mobility Ozone resistance Chemical resistance Fatigue resistance Excellent appearance
- Application Areas:Engine hood parts Automotive sector Automotive interior equip Car exterior decoration Outdoor applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Brittle temperature | ASTMD746 | -52.0 | °C | |
ISO812 | -52.0 | °C |
ageing | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
The rate of change in tensile strength in air | 100°C,1008hr | ASTMD573 | -3.0 | % |
100°C,1008hr | ISO188 | -3.0 | % | |
ChangeinUltimateElongationAir | 100°C,1008hr | ASTMD573 | -10 | % |
ChangeinDurometerHardnessAir | ShoreA,100°C,1008hr | ASTMD573 | 2.0 | |
ChangeinShoreHardnessinAir | ShoreA,100°C,1008hr | ISO188 | 2.0 |
elastomer | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress transverse flow rate | 100%Strain,23°C | ASTMD412 | 2.30 | Mpa |
100%Strain,23°C | ISO37 | 2.30 | Mpa | |
Tensile strength - transverse flow rate | Break,23°C | ASTMD412 | 6.60 | Mpa |
Tensile strength TD | Break,23°C | ISO37 | 6.60 | Mpa |
Elongation rate - lateral flow rate | Break,23°C | ASTMD412 | 490 | % |
Break,23°C | ISO37 | 490 | % | |
Compression permanent deformation 2 | 70°C,22hr | ASTMD395B | 41 | % |
100°C,70hr | ASTMD395B | 53 | % | |
Compression permanent deformation 3 | 70°C,22hr | ISO815 | 41 | % |
100°C,70hr | ISO815 | 53 | % |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,15sec,23°C | ISO868 | 65 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.