Need Help? Contact Us service@plas.com
Get App

TPU Desmopan®  1485A COVESTRO GERMANY

115
  • Unit Price:
    $4292 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    46.6MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:--
  • Application Areas:corrugated pipe Engineering accessories Joint Hose
  • Color:--
  • Grade:Extrusion grade

Technical Data Sheet Compare

Mechanical performanceTest ConditionTest MethodTest ResultUnit
Hardness AASTM D2240/ISO 86886Shore A
Hardness DASTM D2240/ISO 86833Shore D
100% modulusASTM D412/ISO 5275Mpa/Psi
300% modulusASTM D412/ISO 5279Mpa/Psi
tear strength ASTM D624/ISO 3478n/mm²
ResilienceASTM D2630/ISO 466246%
Wear and tear lossISO 464919mm³
Compression deformation rateISO 81536%
Compression deformation rateISO 81511%
Tensile strainBreak, 23°CDIN 53504700%
Tensile Storage Modulus-20°CISO 6721290Mpa
Tensile Storage Modulus20°CISO 672131.0Mpa
Tensile Storage Modulus60°CISO 672121.0Mpa
Tensile stress 2Break, 23°CDIN 5350445.0Mpa
Tensile stress 2100% Strain, 23°CDIN 535045.20Mpa
Tensile stress 2300% Strain, 23°CDIN 535049.00Mpa
Wear resistance 3ISO 464930.0mm³
elastomerTest ConditionTest MethodTest ResultUnit
Rebound ResilienceISO 466244%
Permanent compression deformation23°C, 72 hrISO 81519%
Permanent compression deformation70°C, 24 hr 3ISO 81540%
Permanent compression deformation70°C, 24 hr 5ISO 81529%
Processing performanceTest ConditionTest MethodTest ResultUnit
Melt Temperature 200-220°C
Mold temperature20°C
injectionTest ConditionTest MethodTest ResultUnit
drying temperature< 80°C
Processing (melt) temperature220 到 240°C
Mold temperature20°C
squeezeTest ConditionTest MethodTest ResultUnit
drying temperature< 80°C
Melt Temperature 200 到 220°C
hardnessTest ConditionTest MethodTest ResultUnit
Shore hardnessShore A, 1 sec, 23°CISO 761984
Shore hardnessShore D, 1 sec, 23°CISO 761933
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.