PA11 Rilsan® G820 ARKEMA FRANCE
223
- Unit Price:
- $25724 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:UV resistance Thermal stability
- Application Areas:Electric wire Profile
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Molten Volume Flow Rate (MVR) | 275°C/2.16 kg | ISO 1133 | 8.00 | cm3/10min |
Shrinkage rate | Across Flow | ISO 294-4 | 0.40 | % |
流量 | ISO 294-4 | 0.20 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO 527-2 | -- | Mpa | |
Tensile stress | Yield | ISO 527-2 | -- | Mpa |
Tensile strain | Yield | ISO 527-2 | -- | % |
Nominal tensile fracture strain | ISO 527-2 | > 50 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45 MPa, Unannealed | ISO 75-2/B | 85.0 | °C |
1.8 MPa, Unannealed | ISO 75-2/A | 73.0 | °C | |
Glass transition temperature 2 | ISO 11357-2 | 101 | °C |
injection | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
drying temperature | 80 | °C | ||
drying time | 4.0 到 6.0 | hr | ||
Processing (melt) temperature | 260 到 300 | °C | ||
Mold temperature | 20 到 80 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam without notch | -30°C | ISO 179/1eU | -- | |
23°C | ISO 179/1eU | -- |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Supporting hardness | Shore D, 15 sec | ISO 7619-1 | 76 |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
transmissivity | ISO 13468 | 92.0 | % | |
Renewable Carbon Conent | CSA LISTED | 64 到 66 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.