PES VERADEL® 3330GF SOLVAY USA
153
- Unit Price:
- $18157 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 11MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | 24hr | % | ASTM D570 | 0.50 |
Shrinkage rate | 23℃ | % | ASTM D955 | 0.30 |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strain at break | 23℃ | % | ASTM D638 | 1.8 |
Impact strength of cantilever beam gap | 23℃ | J/m | ASTM D256 | |
Tensile modulus | 23℃ | MPa | ASTM D638 | 8890 |
tensile strength | 23℃ | MPa | ASTM D638 | |
Bending modulus | 23℃ | MPa | ASTM D790 | 8890 |
bending strength | 23℃ | MPa | ASTM D790 |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.82Mpa | ℃ | ASTM D648 | 215 |
Coefficient of thermal expansion | cm/cm/℃ | ASTM D696 | 0.000025 | |
Glass transition temperature | ℃ | DSC | 223 | |
Flame retardancy | 0.80mm | 级 | UL-94 | V0 |
Maximum continuous operating temperature | ℃ | ASTM D794 | ||
Oxygen index | % | ASTM D2863 | 42 |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistance | ohms | ASTM D257 | ||
Insulation strength | kV/mm | ASTM D149 | ||
Volume resistance | ohm-cm | ASTM D257 | ||
Relative track index | V | ASTM D3638 | 150 | |
Arc resistance | sec | ASTM D495 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.