PEEK LNP™ THERMOCOMP™  LC006EX1-BKNAT SABIC INNOVATIVE NANSHA

126
  • Unit Price:
    $72628 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    30MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:--
  • Application Areas:--
  • Color:--
  • Grade:Injection grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9550.10%
Shrinkage rateTD:24hrASTMD9550.40%
Shrinkage rateTD:24hrISO294-40.40%
Shrinkage rateMD:24hrISO294-40.12%
Water absorption rate24hr,50%RHASTMD5700.080%
Water absorption rateEquilibrium,23°C,50%RHISO620.070%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus 2ASTMD63830800Mpa
Tensile modulusISO527-2/124700Mpa
Tensile strengthBreakASTMD638226Mpa
Tensile stressBreakISO527-2230Mpa
elongationBreakASTMD6381.5%
Tensile strainBreakISO527-21.5%
Bending modulusASTMD79020200Mpa
Bending modulusISO17824300Mpa
bending strength ASTMD790325Mpa
Bending stressISO178347Mpa
friction coefficientDynamicASTMD3702Modified0.30
friction coefficientStaticASTMD3702Modified0.32
Wear factor - WasherASTMD3702Modified55.010^-10in^5-min/ft-lb-hr
Thermal performanceTest ConditionTest MethodTest ResultUnit
Linear coefficient of thermal expansionMD:-40to40°CASTME8311.2E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CISO11359-21.2E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8312.9E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CISO11359-22.9E-05cm/cm/°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTMD648>299°C
Hot deformation temperature 40.45MPa,Unannealed,64.0mmSpanISO75-2/Bf>240°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD648>299°C
Hot deformation temperature 41.8MPa,Unannealed,64.0mmSpanISO75-2/Af>240°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Suspended wall beam gap impact strength 323°CISO180/1A7.8kJ/m²
UnnotchedIzodImpactStrength323°CISO180/1U43kJ/m²
Dart impact equipped with measuring instruments23°C,EnergyatPeakLoadASTMD376312.5J
flammabilityTest ConditionTest MethodTest ResultUnit
FlameRating0.77mm,TestingbySABICUL94V-0
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.