Need Help? Contact Us service@plas.com
Get App

EVA TAISOX®  7350F FPC TAIWAN

155
  • Unit Price:
    $2951 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    50MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:Easy to process optical performance High toughness
  • Application Areas:packing Packaging film film currency Sanitary products
  • Color:--
  • Grade:Thin film grade

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Density/specific gravityASTMD15050.938g/cm³
Melt mass flow rate190°C/2.16kgASTMD12381.8g/10min
Vinyl acetate content18.0wt%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile strengthYieldASTMD6384.41Mpa
Tensile strengthBreakASTMD63814.7Mpa
elongationBreakASTMD638800%
Bending modulusASTMD79039.2Mpa
friction coefficientBlown FilmASTMD18940.50
Thermal performanceTest ConditionTest MethodTest ResultUnit
Brittle temperatureASTMD746-70.0°C
Vicat softening temperatureASTMD152560.0°C
Melting temperature84.0°C
filmTest ConditionTest MethodTest ResultUnit
Film thickness - tested30µm
Available film thickness1.2-5.9mil(30-150µ
Secant modulus1%Secant,MD:30μm,Blown FilmASTMD88234.3Mpa
Secant modulus1%Secant,TD:30μm,Blown FilmASTMD88237.3Mpa
Tensile strengthMD:Yield,30μm,Blown FilmASTMD8823.92Mpa
Tensile strengthTD:Yield,30μm,Blown FilmASTMD8822.94Mpa
Tensile strengthMD:Break,30μm,Blown FilmASTMD88227.5Mpa
Tensile strengthTD:Break,30μm,Blown FilmASTMD88224.5Mpa
elongationMD:Break,30μm,Blown FilmASTMD882500%
elongationTD:Break,30μm,Blown FilmASTMD882600%
Falling hammer impact30μm,Blown FilmASTMD1709650g
Elmondov tear strengthMD:30μm,Blown FilmASTMD192212g
Elmondov tear strengthTD:30μm,Blown FilmASTMD192229g
hardnessTest ConditionTest MethodTest ResultUnit
Shore hardnessShore AASTMD22408838
optical performance Test ConditionTest MethodTest ResultUnit
gloss45°,30.0μm,Blown FilmASTMD245790
Haze30.0μm,Blown FilmASTMD10033.0%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.