TPE Hytrel® 3078 DUPONT USA
238
- Unit Price:
- $10500 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:--
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Taber wear amount | H 18轮 | ASTM D-1044 | 90 | mg/1000rev |
CS-17轮 | ASTM D-1044 | 2 | mg/1000rev |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hardness tester hardness | ASTM D-2240 | 30 | ||
Rubbing modulus | 23℃ | ASTM D-790 | 28 | Mpa |
Ezo impact strength | 23℃ | ASTM D-256 | 不破裂 | J/m |
Fracture tensile force | ASTM D-638 | 26.2 | Mpa | |
Initial tear resistance performance | ASTM D-1004 | 77 | kN/m | |
Fracture elongation | ASTM D-638 | 700 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
melting point | ASTM D-3418 | 170 | °C | |
Thermal distortion temperature | @0.5Mpa | ASTM D-638 | 46 | °C |
vicat softening point | ASTM D-1525 | 83 | °C | |
Thermal distortion temperature | @0.18Mpa | ASTM D-638 | N/A | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Stretching force | 5%伸长 | ASTM D-638 | 1.3 | Mpa |
10%伸长 | ASTM D-638 | 2.1 | Mpa |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
24-hour water absorption rate | ASTM D-570 | 3 | % |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Wear resistant and flexible incision growth performance | ASTM D-1052 | >1×10 | ||
Melt index | ASTM D-1238 | 5.0 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.