Need Help? Contact Us service@plas.com
Get App

PBT LNP™ LUBRICOMP™  WL004 GY03565 SABIC INNOVATIVE US

110
  • Unit Price:
    $3989 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    50MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:High rigidity high strength
  • Application Areas:Home appliance components Automotive Applications
  • Color:--
  • Grade:--

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9552.1to2.4%
Shrinkage rateTD:24hrASTMD9552.1to2.4%
Shrinkage rateTD:24hrISO294-42.1to2.3%
Shrinkage rateMD:24hrISO294-42.4to2.5%
Water absorption rate24hr,50%RHASTMD5700.051%
Water absorption rateEquilibrium,23°C,50%RHISO620.080%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile stressBreakISO527-245.0Mpa
Tensile strainBreakISO527-28.4%
Tensile modulusISO527-2/12450Mpa
elongationBreakASTMD6389.8%
Bending modulusASTMD7902410Mpa
Bending modulusISO1782390Mpa
bending strength ASTMD79078.7Mpa
Bending stressISO17877.1Mpa
friction coefficientDynamicASTMD3702Modified0.33
friction coefficientStaticASTMD3702Modified0.24
Tensile modulus 2ASTMD6382410Mpa
Tensile strengthBreakASTMD63849.0Mpa
Wear factor - WasherASTMD3702Modified58.010^-10in^5-min/ft-lb-hr
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature 41.8MPa,Unannealed,64.0mmSpanISO75-2/Af61.0°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD64855.0°C
Linear coefficient of thermal expansionMD:-40to40°CISO11359-29E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CASTME8319.6E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CISO11359-29.6E-05cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8319E-05cm/cm/°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Multi axis Instrumented Impact EnergyISO6603-20.500J
Suspended wall beam gap impact strength 323°CISO180/1A3.6kJ/m²
UnnotchedIzodImpactStrength323°CISO180/1U30kJ/m²
Dart impact equipped with measuring instruments23°C,EnergyatPeakLoadASTMD37630.960J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.