PBT LNP™ LUBRICOMP™ WFL4036 SABIC INNOVATIVE US
145
Unit Price:$8399 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan|wear resistant
- Application Areas:Plastic bag|Automotive Applications|Industrial applications
- Color:--
- Grade:Enhanced level
Technical Data Sheet
Physical | Test Condition | Test Method | Test Result |
---|---|---|---|
Moisture Absorption | 24hr,50%RH | ASTMD570 | 0.040 % |
平衡,23°C,50%RH | ISO62 | 0.040 % | |
Modeling Shrinkage | MD:24小时 | ASTMD955 | 0.10to0.30 % |
TD:24hr | ASTMD955 | 0.50to1.0 % | |
TD:24小时 | ISO294-4 | 0.50to1.0 % | |
MD:24小时 | ISO294-4 | 0.10to0.30 % |
Thermal Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | 1.8MPa,未退火,3.20mm | ASTMD648 | 218 °C |
1.8MPa,未退火,64.0mm跨距 | ISO75-2/Af | 214 °C | |
Linear thermal expansion coefficient | MD:-40到40°C | ASTME831 | 3.9E-05 cm/cm/°C |
MD:-40到40°C | ISO11359-2 | 3.9E-05 cm/cm/°C | |
TD:-40到40°C | ASTME831 | 6.7E-05 cm/cm/°C | |
TD:-40到40°C | ISO11359-2 | 6.7E-05 cm/cm/°C |
Mechanical Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Modulus | ASTMD638 | 10300 Mpa | |
ISO527-2/1 | 10600 Mpa | ||
Tensile Strength | 断裂 | ASTMD638 | 118 Mpa |
Tensile Stress | 断裂 | ISO527-2 | 118 Mpa |
Tensile Elongation | 断裂 | ASTMD638 | 2.3 % |
Tensile Strain | 断裂 | ISO527-2 | 2.2 % |
Flexural Modulus | ASTMD790 | 10200 Mpa | |
ISO178 | 10000 Mpa | ||
Flexural Strength | ASTMD790 | 193 Mpa | |
Flexural Stress | ISO178 | 187 Mpa | |
Coefficient of Friction | Dynamic | ASTMD3702Modified | 0.57 |
Static | ASTMD3702Modified | 0.41 | |
Specific Wear Rate | ASTMD3702Modified | 42.0 10^-10in^5-min/ft-lb-hr |
Impact Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Notched Izod Impact Strength | 23°C | ISO180/1A | 9.2 kJ/m² |
UnnotchedIzodImpactStrength3 | 23°C | ISO180/1U | 43 kJ/m² |
Instrumented Dart Impact | 23°C,EnergyatPeakLoad | ASTMD3763 | 13.7 J |
Multi-Axial Instrumented Impact Energy | ISO6603-2 | 2.61 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.