PBT VALOX™ 310SE0 SABIC INNOVATIVE US
176
Unit Price:$3977 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant
- Application Areas:Electrical field Electronic field Home appliance components switch Shell Spool
- Color:--
- Grade:Injection grade
Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
收缩率 | MD:--2 | 内部方法 | 1.1to1.8 | % |
MD:--3 | 内部方法 | 1.5to2.3 | % | |
MD:--4 | 内部方法 | 0.90to1.6 | % | |
MD:3.20mm | 内部方法 | 1.5to2.3 | % | |
TD:--2 | 内部方法 | 0.90to1.9 | % | |
TD:--4 | 内部方法 | 1.0to1.7 | % | |
TD:--3 | 内部方法 | 1.6to2.4 | % | |
吸水率 | 饱和,23°C | ISO62 | 0.36 | % |
平衡,23°C,50%RH | ISO62 | 0.080 | % | |
熔体质量流动速率 | 250°C/2.16kg | ASTMD1238 | 8.6 | g/10min |
熔体体积流动速率 | 250°C/2.16kg | ISO1133 | 8.00 | cm3/10min |
密度 / 比重 | ISO1183 | 1.40 | g/cm³ | |
ASTMD792 | 1.40 | g/cm³ | ||
特定体积 | ASTMD792 | 0.710 | cm³/g |
机械性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
弯曲模量7 | 50.0mmSpan | ASTMD790 | 2620 | Mpa |
弯曲强度8,9 | ISO178 | 90.0 | Mpa | |
拉伸应变6 | Yield | ASTMD638 | 20 | % |
弯曲模量8 | ISO178 | 2600 | Mpa | |
拉伸强度6 | Break | ASTMD638 | 58.0 | Mpa |
Yield | ASTMD638 | 58.0 | Mpa | |
伸长率6 | 断裂 | ASTMD638 | 20 | % |
FlexuralStrength7 | Yield,50.0mmSpan | ASTMD790 | 101 | Mpa |
拉伸模量5 | ASTMD638 | 2820 | Mpa | |
泰伯耐磨性 | 1000Cycles,1000g,CS-17转轮 | 内部方法 | 19.0 | mg |
拉伸应力 | 屈服 | ISO527-2/50 | 55.0 | Mpa |
断裂 | ISO527-2/50 | 40.0 | Mpa | |
拉伸应变 | 屈服 | ISO527-2/50 | 6.0 | % |
断裂 | ISO527-2/50 | 20 | % | |
拉伸模量 | ISO527-2/1 | 2800 | Mpa |
热性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
热变形温度 | 1.8MPa,未退火,100mm跨距12 | ISO75-2/Ae | 60.0 | °C |
1.8MPa,未退火,64.0mm跨距13 | ISO75-2/Af | 71.0 | °C | |
1.8MPa,未退火,3.20mm | ASTMD648 | 74.0 | °C | |
1.8MPa,未退火,6.40mm | ASTMD648 | 71.0 | °C | |
0.45MPa,未退火,6.40mm | ASTMD648 | 162 | °C | |
线形热膨胀系数 | MD:23to60°C | ISO11359-2 | 1E-04 | cm/cm/°C |
TD:-40到40°C | ASTME831 | 7.9E-05 | cm/cm/°C | |
TD:-40to40°C | ISO11359-2 | 7.3E-05 | cm/cm/°C | |
TD:23to60°C | ISO11359-2 | 1E-04 | cm/cm/°C | |
MD:-40to40°C | ASTME831 | 7.9E-05 | cm/cm/°C | |
MD:60to138°C | ASTME831 | 1.3E-04 | cm/cm/°C | |
MD:-40to40°C | ISO11359-2 | 7.6E-05 | cm/cm/°C | |
RTIElec | UL746 | 120 | °C | |
RTIImp | UL746 | 120 | °C | |
RTIStr | UL746 | 140 | °C | |
导热系数 | ISO8302 | 0.24 | W/m/K | |
BallPressureTest | 125°C | IEC60695-10-2 | Pass | |
维卡软化温度 | ASTMD152514 | 165 | °C | |
-- | ISO306/A50 | 212 | °C | |
-- | ISO306/B50 | 165 | °C | |
-- | ISO306/B120 | 165 | °C | |
热变形温度12 | 0.45MPa,Unannealed,100mmSpan | ISO75-2/Be | 135 | °C |
电气性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
高电弧燃烧指数 | HAI | UL746 | PLC0 | |
高电压电弧起痕速率 | HVTR | UL746 | PLC4 | |
高压电弧抗点燃指数 | PLC | UL746 | PLC6 | |
相比耐漏电起痕指数 | CTI | UL746 | PLC3 | |
热丝引燃 | HWI | UL746 | PLC2 | |
耐电弧性16 | ASTMD495 | PLC6 | ||
相对电容率 | 50Hz | IEC60250 | 2.90 | |
60Hz | IEC60250 | 2.90 | ||
100Hz | IEC60250 | 3.10 | ||
1MHz | IEC60250 | 2.80 | ||
漏电起痕指数 | -- | IEC60112 | 175 | V |
解决方案B | IEC60112 | 100 | V | |
耗散因数 | 50Hz | IEC60250 | 1E-03 | |
60Hz | IEC60250 | 1E-03 | ||
100Hz | IEC60250 | 2E-03 | ||
1MHz | IEC60250 | 0.010 | ||
介电强度 | 1.60mm,在油中 | ASTMD149 | 22 | KV/mm |
3.20mm,inAir | ASTMD149 | 18 | KV/mm | |
0.800mm,在油中 | IEC60243-1 | 31 | KV/mm | |
1.00mm15 | IEC60243-1 | 18 | KV/mm | |
1.60mm,在油中 | IEC60243-1 | 24 | KV/mm | |
3.20mm,在油中 | IEC60243-1 | 15 | KV/mm | |
表面电阻率 | IEC60093 | >1.0E+15 | ohms | |
体积电阻率 | IEC60093 | >1.0E+15 | ohms·cm |
冲击性能 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
装有测量仪表的落镖冲击 | 23°C,TotalEnergy | ASTMD3763 | 200 | J |
悬壁梁缺口冲击强度11 | -30°C | ISO180/1A | 3.0 | kJ/m² |
23°C | ISO180/1A | 5.0 | kJ/m² | |
无缺口伊佐德冲击强度11 | -30°C | ISO180/1U | NoBreak | |
23°C | ISO180/1U | NoBreak | ||
简支梁缺口冲击强度 | 23°C10 | ISO179/1eA | 8.0 | kJ/m² |
23°C | ISO179/2C | 4.0 | kJ/m² | |
-30°C10 | ISO179/1eA | 4.0 | kJ/m² | |
悬壁梁缺口冲击强度 | -30°C | ASTMD256 | 22 | J/m |
23°C | ASTMD256 | 37 | J/m | |
23°C | ASTMD4812 | 1600 | J/m | |
简支梁无缺口冲击强度10 | -30°C | ISO179/1eU | NoBreak | |
23°C | ISO179/1eU | NoBreak |
硬度 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
洛氏硬度 | R级 | ISO2039-2 | 120 | |
球压硬度 | H358/30 | ISO2039-1 | 105 | Mpa |
可燃性 | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL阻燃等级 | 0.71mm | UL94 | V-0 | |
3.0mm | UL94 | 5VA | ||
灼热丝易燃指数 | 1.0mm | IEC60695-2-12 | 960 | °C |
极限氧指数 | ISO4589-2 | 30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.