PPO FLEX NORYL™ WCD825-BK1066 SABIC INNOVATIVE SHANGHAI
113
- Unit Price:
- $3119 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High barrier UV resistance
- Application Areas:Electronic and electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 250°C/10.0kg | ASTMD1238 | 16 | g/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
crack | CCP METHOD | 23.0 | Mpa | |
ISO527-2/50 | 16.0 | Mpa | ||
CCP METHOD | 310 | % | ||
ISO527-2/50 | 250 | % | ||
Fracture 3 | ASTMD638 | 260 | % | |
Fracture 1 | ASTMD638 | 16.0 | Mpa | |
Fracture, 136 ° C2 | CCP METHOD | 22.0 | Mpa | |
Fracture, 136 ° C4 | CCP METHOD | 250 | % | |
100mm span | ASTMD790 | 65.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
HeatDeformation6 | 121°C | CCP METHOD | 5.0 | % |
Brittle temperature | ASTMD746 | <-40.0 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation factor | 1MHz | ASTMD150 | 7E-03 | |
Dielectric strength | 2.00mm,in Oil | IEC60243-1 | 25 | KV/mm |
Dielectric constant | 1MHz | ASTMD150 | 2.40 | |
Volume resistivity | ASTMD257 | 1.9E+16 | ohms·cm | |
Leakage Trace Index | IEC60112 | 600 | V |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shore hardness | Shore A,30sec | ASTMD2240 | 85 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning wire flammability index | 3.00mm | IEC60695-2-12 | 850 | °C |
Extreme Oxygen Index | ISO4589-2 | 27 | % | |
VW-1 | CCP METHOD | Pass | ||
Hot filament ignition temperature | 3.00mm | IEC60695-2-13 | 825 | °C |
Smoke density | Flame,0.5mmplaque,Ds,max | ASTME662 | 110 | |
Non-Flame,0.5mmplaque,Ds,max | ASTME662 | 47 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.