PPS Torelina® A610MX46 TORAY SHENZHEN
127
- Unit Price:
- $4470 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 11MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Glass fiber reinforced Flame retardant
- Application Areas:Electrical applications Lighting fixtures
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Flowing Long | 320℃,98MPa,1mm厚 | 东丽法 | 120 | |
Shrinkage rate | Flow | 东丽法 | 0.25 | % |
垂重方向 | 东丽法 | 0.70 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
friction coefficient | 对钢 | ASTM D-1894 | 0.30 | |
tensile strength | ASTM D-638 | 1.0 | % | |
Limit PV value | 东丽法 | 815 | KJ/m | |
abrasion | ASTM D-1044 | 70 | mg/1000回 | |
Tensile strength | ASTM D-638 | 145 | Mpa | |
hardness | ASTM D-785 | 123 | 洛氏 | |
bending strength | ASTM D-790 | 200 | Mpa | |
impact strength | Notched23℃ | ASTM D-256 | 110 | J/m |
Unnotched23℃ | ASTM D-256 | 27 | KJ/m | |
Curved elastic body | ASTM D-790 | 19.6 | GPa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Line expansion coefficient | Flow | ASTM D-696 | 1.6 | |
垂重方向 | ASTM D-696 | 2.4 | ||
Combustibility | UL-94 | V-0 | ||
Hot deformation temperature | 1.82MPa | ASTM D-648 | >260 | °C |
Rongdian | DSC | 278 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Arc resistance W level | ASTM D-495 | 127 | 秒 | |
Induced positive connection | 10 | ASTM D-150 | 0.002 | |
permittivity | 10 | ASTM D-150 | 5.8 | |
Insulation breakdown voltage | ASTM D-149 | 15 | MV/m | |
Fracture strength | ASTM D-732 | 65 | ||
Inherent resistance of volume | ASTM D-257 | 10 | Ω.m |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | ASTM D-570 | 0.02 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.