PPS INFINO® XP-2130A Samsung Cheil South Korea
175
- Unit Price:
- $5769 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 12.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:enhance Flame retardant Filler: Glass fiber reinf
- Application Areas:Connector Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Density/specific gravity | ASTMD792 | 1.65 | g/cm³ | |
ISO1183 | 1.65 | g/cm³ | ||
Melt mass flow rate | 315°C/5.0kg | ASTMD1238 | 120 | g/10min |
315°C/5.0kg | ISO1133 | 120 | g/10min | |
Shrinkage rate | MD:3.20mm | ASTMD955 | 0.30to1.2 | % |
TD:3.20mm | ASTMD955 | 0.30to1.2 | % | |
TD:3.20mm | ISO2577 | 0.30to1.2 | % | |
MD:3.20mm | ISO2577 | 0.30to1.2 | % | |
Ash Content | -- | ISO3451 | 30 | % |
-- | ASTMD5630 | 30 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus 2 | ASTMD638 | 5900 | Mpa | |
Tensile modulus | ISO527-2/5 | 8000 | Mpa | |
Tensile strength 2 | Yield | ASTMD638 | 140 | Mpa |
Tensile stress | Yield | ISO527-2/5 | 128 | Mpa |
Tensile strength 2 | Break | ASTMD638 | 130 | Mpa |
Tensile stress | Break | ISO527-2/5 | 115 | Mpa |
Elongation rate 2 | Break | ASTMD638 | 3.0 | % |
Tensile strain | Break | ISO527-2/5 | 3.0 | % |
Bending modulus 3 | ASTMD790 | 9800 | Mpa | |
ISO178 | 10000 | Mpa | ||
Bending strength 3 | ASTMD790 | 200 | Mpa | |
Bending stress 3 | ISO178 | 190 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 282 | °C |
0.45MPa,Unannealed,4.00mm | ISO75-2/B | 289 | °C | |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 275 | °C | |
1.8MPa,Unannealed,4.00mm | ISO75-2/A | 275 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam gap 4 | 23°C | ISO179/1eA | 11 | kJ/m² |
Impact strength of cantilever beam gap | 23°C,3.18mm | ASTMD256 | 88 | J/m |
23°C,6.35mm | ASTMD256 | 79 | J/m | |
Suspended wall beam gap impact strength 4 | 23°C | ISO180/1A | 11 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Scale | ASTMD785 | 120 | |
R-Scale | ISO2039-2 | 116 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FlameRating | 0.75mm | UL94 | V-0 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.