LCP VECTRA® V400P CELANESE USA
108
- Unit Price:
- $6222 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 50MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Chemical resistance transparent Halogen-free Barrier resin Flame retardant
- Application Areas:film
- Color:--
- Grade:Extrusion grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | Equilibrium, 23°C, 50% RH | ISO 62 | 0.040 | % |
Melt flow rate | 230°C/2.16 kg | 内部方法 | 14 | g/10 min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress | Break | ISO 527-2/1A/5 | 151 | Mpa |
Tensile strain | Break | ISO 527-2/1A/5 | 1.6 | % |
Tensile modulus | ISO 527-2/1A/1 | 14400 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8 MPa, Unannealed | ISO 75-2/A | 111 | °C |
Glass transition temperature 4 | ISO 3146 | 110 | °C |
film | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen Permeability | 23°C 2 | DIN 53380-3 | 1.4 | cc-25µm/m²-day-atm |
23°C 3 | DIN 53380-3 | 1.3 | cc-25µm/m²-day-atm | |
Water Vapor Permeability | 38°C | DIN 53122 | 0.400 | g-25µm/(m² day-atm) |
injection | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
drying temperature | 90 | °C | ||
Suggested maximum moisture content | 0.010 | % | ||
Processing (melt) temperature | 225 到 235 | °C | ||
drying time | 8.0 到 24 | hr | ||
Temperature at the rear of the barrel | 185 到 195 | °C | ||
Temperature in the middle of the barrel | 205 到 215 | °C | ||
Temperature at the front of the material cylinder | 205 到 215 | °C | ||
Spray nozzle temperature | 200 到 210 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.