PC/ABS CYCOLOY™ C2950HF-WH8082 SABIC INNOVATIVE NANSHA
125
- Unit Price:
- $2840 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 19MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant High mobility High impact resistance High temperature resistan heat-resisting
- Application Areas:Electrical field Electronic field Household appliances Household appliances Automotive sector
- Color:--
- Grade:Flame retardant and high temperature resistant grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 260°C/2.16kg | ASTMD1238 | 22 | g/10min |
Shrinkage rate | MD:3.20mm | 内部方法 | 0.40to0.60 | % |
TD:3.20mm | 内部方法 | 0.40to0.60 | % | |
Water absorption rate | 24hr | ASTMD570 | 0.10 | % |
Equilibrium,23°C | ASTMD570 | 0.40 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength 2 | Yield | ASTMD638 | 64.1 | Mpa |
Elongation rate 2 | Yield | ASTMD638 | 5.0 | % |
Break | ASTMD638 | 40 | % | |
Bending modulus 3 | 100mmSpan | ASTMD790 | 2590 | Mpa |
FlexuralStrength3 | Yield,100mmSpan | ASTMD790 | 96.5 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
thermal conductivity | ASTMC177 | 0.20 | W/m/K | |
RTIElec | UL746 | 85.0 | °C | |
Evolution Calendar intelligent importer | UL746 | 85.0 | °C | |
RTIStr | UL746 | 85.0 | °C | |
Hot deformation temperature | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 102 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 87.8 | °C | |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 93.3 | °C | |
Vicat softening temperature | ASTMD15254 | 113 | °C | |
Linear coefficient of thermal expansion | MD:-30to30°C | ASTMD696 | 7.2E-05 | cm/cm/°C |
TD:-30to30°C | ASTMD696 | 7.2E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dissipation factor | 50Hz | ASTMD150 | 5.2E-03 | |
60Hz | ASTMD150 | 5.2E-03 | ||
1MHz | ASTMD150 | 7.1E-03 | ||
Arc resistance 5 | ASTMD495 | PLC6 | ||
Compared to the anti leakage trace index | CTI | UL746 | PLC2 | |
High arc combustion index | HAI | UL746 | PLC0 | |
High voltage arc tracing rate | HVTR | UL746 | PLC3 | |
Hot wire ignition | HWI | UL746 | PLC2 | |
Surface resistivity | ASTMD257 | >1.0E+16 | ohms | |
Volume resistivity | ASTMD257 | 1.6E+17 | ohms·cm | |
Dielectric strength | 3.20mm,inOil | ASTMD149 | 24 | KV/mm |
Dielectric constant | 50Hz | ASTMD150 | 2.80 | |
60Hz | ASTMD150 | 2.80 | ||
1MHz | ASTMD150 | 2.70 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dart impact equipped with measuring instruments | 23°C,EnergyatPeakLoad | ASTMD3763 | 54.2 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Scale | ASTMD785 | 121 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 0.76mm | UL94 | V-2 | |
1.5mm | UL94 | V-0 | ||
2.5mm | UL94 | 5VB | ||
3.4mm | UL94 | 5VA | ||
Extreme Oxygen Index | ASTMD2863 | 30 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.