PC EMERGE™ 8600-20 IC7700035 STYRON TAIWAN
200
- Unit Price:
- $3294 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 55.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant High mobility Bromine free
- Application Areas:Electrical/Electronic App Electrical field Electrical enclosure
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt mass flow rate | 300°C/1.2kg | ISO1133 | 20 | g/10min |
Shrinkage rate | ISO294-4 | 0.50to0.70 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
tensile strength | Yield,4.00mm,InjectionMolded | ISO527-2/50 | 60.0 | Mpa |
Tensile stress | Break,4.00mm,Injection | ISO527-2/50 | 58.0 | Mpa |
TensileStrain | Yield,4.00mm,InjectionMolded | ISO527-2/50 | 6.0 | % |
Tensile strain | Break,4.00mm,Injection | ISO527-2/50 | 100 | % |
Bending modulus 2 | 4.00mm,InjectionMolded | ISO178 | 2400 | Mpa |
Bending strength 2 | 4.00mm,InjectionMolded | ISO178 | 94.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 136 | °C |
1.8MPa,Unannealed | ISO75-2/A | 122 | °C | |
Vicat softening temperature | -- | ISO306/A120 | 150 | °C |
-- | ISO306/B50 | 143 | °C | |
Ball pressure temperature | IEC60335-1 | >125 | °C | |
Linear coefficient of thermal expansion | MD:-40to82°C | ASTMD696 | 6.5E-05 | cm/cm/°C |
RTIElec | UL746 | 125 | °C | |
Evolution Calendar intelligent importer | UL746 | 125 | °C | |
RTIStr | UL746 | 125 | °C |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | R-Scale,4.00mm | ISO2039-2 | 123 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
FlameRating3 | 1.5mm | UL94 | V-0 | |
GlowWireIgnitionTemperature3 | 1.0mm | IEC60695-2-13 | 960 | °C |
Extreme Oxygen Index 3 | ISO4589-2 | 35 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.