Technical Data Sheet
Compare
physical property | Test Condition | Test Method | Test Result | Unit |
---|
Melt mass flow rate | 300°C/1.2kg | ASTMD1238 | 8.0 | g/10min |
Shrinkage rate | MD | ASTMD955 | 0.50到0.70 | % |
Water absorption rate | 23°C,24hr | ASTMD570 | 0.15 | % |
Water absorption rate | Equilibrium,23°C,50%RH | ASTMD570 | 0.32 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Bending modulus | | ASTMD790 | 2410 | Mpa |
bending strength | | ASTMD790 | 96.0 | Mpa |
Wear resistance - AngelinHaze1 | | Kg/m | 45 | % |
Tensile modulus | | ASTMD638 | 2410 | Mpa |
Tensile strength | Yield | ASTMD638 | 60.0 | Mpa |
Tensile strength | Break | ASTMD638 | 72.0 | Mpa |
elongation | Yield | ASTMD638 | 6.0 | % |
elongation | Break | ASTMD638 | 150 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 0.45MPa,Annealed,4.00mm | ASTMD648 | 144 | °C |
Hot deformation temperature | 1.8MPa,Unannealed,4.00mm | ASTMD648 | 128 | °C |
Hot deformation temperature | 1.8MPa,Annealed,4.00mm | ASTMD648 | 141 | °C |
Vicat softening temperature | | ASTMD15254 | 150 | °C |
Ball pressure temperature | | IEC60598-1 | >125 | °C |
Linear coefficient of thermal expansion | MD:-40to82°C | ASTMD696 | 6.8E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Volume resistivity | 23°C | ASTMD257 | 2E+17 | ohms·cm |
Dielectric strength | | ASTMD149 | 17 | KV/mm |
Dielectric constant | 60Hz | ASTMD150 | 3.00 | |
Dissipation factor | 60Hz | ASTMD150 | 1E-03 | |
Leakage Trace Index | 2.00mm | IEC60112 | 250 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Suspended wall beam notch impact strength 2 | 23°C,3.20mm | ASTMD256 | 900 | J/m |
Cantilever beam without notch impact strength | 23°C | ASTMD256 | 无断裂 | |
Dart impact equipped with measuring instruments 3 | 23°C,3.20mm,TotalEnergy | ASTMD3763 | 89.0 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Rockwell hardness | M-Scale | ASTMD785 | 73 | |
Rockwell hardness | R-Scale | ASTMD785 | 118 | |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|
Refractive index | | ASTMD542 | 1.586 | |
transmissivity | | ASTMD1003 | 89.0 | % |
Haze | | ASTMD1003 | 0.70到1.5 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 0.500mm | UL94 | V-2 | |
UL flame retardant rating | 1.60mm | UL94 | V-2 | |
UL flame retardant rating | 2.50mm | UL94 | V-2 | |
UL flame retardant rating | 3.00mm | UL94 | V-2 | |
Hot filament ignition temperature 5 | 2.00mm | IEC60695-2-13 | 850 | °C |
Extreme Oxygen Index | | ASTMD2863 | 26 | % |
Average degree of combustion | | ASTMD635 | 3 | CM |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.