PC Makrolon® 1800 COVESTRO GERMANY
190
- Unit Price:
- $7209 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Thermal stability High temperature resistan high viscosity
- Application Areas:Electrical applications Connector Automotive Applications
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt index (volume) | 330℃/2.16kg | ISO 1133 | 10/10 | CM |
Melt index (mass) | 330℃/2.16kg | ISO 1133 | 10/10 | g/(10min) |
Shrinkage rate | Flow | ISO 2577 | 0.85 | % |
垂直Flow | ISO 2577 | 0.85 | % | |
Water absorption | 23℃Saturation值 | ISO 62 | 0.4 | % |
Hygroscopicity | 23℃/50%相对湿度,Saturation值 | ISO 62 | 0.2 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | 1mm/mim | ISO 527-1-2 | 2300 | Mpa |
Yield stress | 50mm/mim | ISO 527-1-2 | 65 | Mpa |
Yield strain | 50mm/mim | ISO 527-1-2 | 7 | % |
Fracture elongation rate | 50mm/mim | ISO 527-1-2 | >50 | % |
Flexural modulus | 2mm/mim | ISO 178 | 2200 | Mpa |
Flexural strength | 5mm/mim | ISO 178 | 95 | Mpa |
Ball scratch hardness | ISO 2309-1 | 115 | N/mm |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.80Mpa | ISO 75-1,-2 | 162/151/160 | °C |
Linear thermal expansion coefficient in flow direction | 23~55℃ | ASTME811 | 0.7 | |
Linear thermal expansion coefficient in the vertical flow direction | 23~55℃ | ASTME811 | 0.7 |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
loss factor | 100Hz/1MHz | 1EC250 | 13/100 |
Processing performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Melt Temperature | ISO 294 | 330 | °C | |
Mold temperature | ISO 294 | 100 | °C | |
Injection temperature | ISO 294 | 200 | mm/g |
Other performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Oxygen index | ISO 4589 | 24 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.