PC LEXAN™ GLX143-NA9C029H SABIC INNOVATIVE US
104
- Unit Price:
- $5908 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 10MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Middle flow Thermal stability
- Application Areas:Electronic display Application in the automo Lighting applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD1 | 内部方法 | 0.50到0.70 | % |
Water absorption rate | Saturation,23°C | ISO62 | 0.35 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.15 | % | |
Melt volume flow rate | 300°C/1.2kg | ISO1133 | 12.0 | cm3/10min |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Bending stress 3 | ISO178 | 90.0 | Mpa | |
Tensile stress | Yield | ISO527-2/50 | 65.0 | Mpa |
Break | ISO527-2/50 | 70.0 | Mpa | |
Tensile strain | Yield | ISO527-2/50 | 6.0 | % |
Break | ISO527-2/50 | 120 | % | |
Tensile modulus | ISO527-2/1 | 2350 | Mpa | |
Bending modulus 2 | ISO178 | 2300 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear coefficient of thermal expansion | MD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C |
TD:23to80°C | ISO11359-2 | 7E-05 | cm/cm/°C | |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 125 | °C | |
thermal conductivity | ISO8302 | 0.20 | W/m/K | |
RTI | UL746 | 125 | °C | |
BallPressure Test | 125°C | IEC60695-10-2 | Pass | |
1.8MPa, unannealed, 64.0mm span of 10 | ISO75-2/Af | 124 | °C | |
-- | ISO306/B50 | 142 | °C | |
ISO306/B120 | 143 | °C | ||
0.45MPa, unannealed, 100mm span 8 | ISO75-2/Be | 136 | °C | |
1.8MPa, unannealed, 100mm span 9 | ISO75-2/Ae | 125 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Relative permittivity | 50Hz | IEC60250 | 2.70 | |
60Hz | IEC60250 | 2.70 | ||
1MHz | IEC60250 | 2.70 | ||
Dissipation factor | 50Hz | IEC60250 | 1E-03 | |
60Hz | IEC60250 | 1E-03 | ||
1MHz | IEC60250 | 0.010 | ||
Dielectric strength | 1.00mm11 | IEC60243-1 | 15 | KV/mm |
3.20mm,in Oil | IEC60243-1 | 17 | KV/mm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Simply supported beam without notch impact strength 5 | -30°C | ISO179/1eU | 无断裂 | |
23°C | ISO179/1eU | 无断裂 | ||
Suspended wall beam notch impact strength 6 | -30°C | ISO180/1A | 12 | kJ/m² |
23°C | ISO180/1A | 70 | kJ/m² | |
Unscented Izod Impact Strength 7 | -30°C | ISO180/1U | 无断裂 | |
23°C | ISO180/1U | 无断裂 | ||
Impact strength of simply supported beam gap 4 | -30°C | ISO179/1eA | 14 | kJ/m² |
23°C | ISO179/1eA | 73 | kJ/m² |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Haze | 2540µm | ASTMD1003 | <0.80 | % |
Refractive index | ISO489 | 1.586 | ||
transmissivity | 3000µm | ASTMD1003 | 89.0 | % |
4000µm | ASTMD1003 | 88.0 | % | |
5000µm | ASTMD1003 | 87.0 | % | |
6000µm | ASTMD1003 | 86.0 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning wire flammability index | 1.00mm | IEC60695-2-12 | 850 | °C |
Extreme Oxygen Index | ISO4589-2 | 25 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.