PC PANLITE® L-1225T TEIJIN JAPAN
141
- Unit Price:
- $3500 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 30MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:--
- Application Areas:Thin walled products Electrical appliances Labor protection equipmen Application in the automo Car headlights container Disposable tableware
- Color:--
- Grade:Transparent level
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | TD:4.00mm | 内部方法 | 0.50to0.70 | % |
MD:4.00mm | 内部方法 | 0.50to0.70 | % | |
Water absorption rate | 23°C,24hr | ISO62 | 0.20 | % |
Melt volume flow rate | 300°C/1.2kg | ISO1133 | 25.0 | cm3/10min |
Density/specific gravity | ISO1183 | 1.20 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Nominal tensile fracture strain | ISO527-2/50 | >50 | % | |
Tensile stress | Yield | ISO527-2/50 | 62.0 | Mpa |
Tensile strain | Yield | ISO527-2/50 | 6.0 | % |
Tensile modulus | ISO527-2/1 | 2400 | Mpa | |
Bending modulus 2 | ISO178 | 2400 | Mpa | |
Bending stress 2 | ISO178 | 95.0 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
RTIElec | 1.5mm | UL746 | 125 | °C |
Evolution Calendar intelligent importer | 1.5mm | UL746 | 115 | °C |
RTIStr | 1.5mm | UL746 | 125 | °C |
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 136 | °C |
1.8MPa,Unannealed | ISO75-2/A | 123 | °C | |
Vicat softening temperature | ISO306/B50 | 142 | °C | |
Linear coefficient of thermal expansion | MD | ISO11359-2 | 7E-05 | cm/cm/°C |
TD | ISO11359-2 | 7E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric strength 3 | IEC60243-1 | 30 | KV/mm | |
Surface resistivity | IEC60093 | >1.0E+15 | ohms | |
Volume resistivity | IEC60093 | >1.0E+15 | ohms·cm | |
Dissipation factor | 100Hz | IEC60250 | 1E-03 | |
1MHz | IEC60250 | 9E-03 | ||
Relative permittivity | 100Hz | IEC60250 | 3.10 | |
1MHz | IEC60250 | 3.00 | ||
Leakage Trace Index | IEC60112 | 250 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of simply supported beam without notch | ISO179 | NoBreak | ||
Charpy Notched Impact Strength | ISO179 | 53 | kJ/m² |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index | ASTMD542 | 1.585 | ||
transmissivity | 3000µm | ASTMD1003 | 88.0 | % |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
UL flame retardant rating | 2.1mm | UL94 | HB | |
0.40mm | UL94 | V-2 | ||
Burning wire flammability index | 1.5mm | IEC60695-2-12 | 825 | °C |
3.2mm | IEC60695-2-12 | 875 | °C | |
Hot filament ignition temperature | 1.5mm | IEC60695-2-13 | 850 | °C |
3.2mm | IEC60695-2-13 | 875 | °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.