PC LEXAN™ 503R-131 SABIC INNOVATIVE SINGAPHORE
209
- Unit Price:
- $2821 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20.5MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High impact resistance High rigidity Glass fiber reinforced enhance
- Application Areas:fibre
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | 内部方法 | 0.20to0.40 | % |
Water absorption rate | 24hr | ASTMD570 | 0.12 | % |
Equilibrium,23°C | ASTMD570 | 0.31 | % | |
Specific volume | ASTMD792 | 0.802 | cm³/g | |
Outdoor applicability | UL746C | f1 |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength 2 | Yield | ASTMD638 | 66.2 | Mpa |
Break | ASTMD638 | 55.2 | Mpa | |
Elongation rate 2 | Yield | ASTMD638 | 8.0 | % |
Break | ASTMD638 | 15 | % | |
Bending modulus 4 | 50.0mmSpan | ASTMD790 | 3450 | Mpa |
Bending strength 4 | Yield,50.0mmSpan | ASTMD790 | 103 | Mpa |
Taber abraser | 1000Cycles,1000g,CS-17Wheel | ASTMD1044 | 11.0 | mg |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Linear coefficient of thermal expansion | MD:-40to95°C | ASTME831 | 3.2E-05 | cm/cm/°C |
Hot deformation temperature | 0.45MPa,Unannealed,6.40mm | ASTMD648 | 146 | °C |
1.8MPa,Unannealed,6.40mm | ASTMD648 | 142 | °C | |
RTIElec | UL746 | 120 | °C | |
Evolution Calendar intelligent importer | UL746 | 110 | °C | |
RTIStr | UL746 | 125 | °C | |
specific heat | ASTMC351 | 1210 | J/kg/°C | |
thermal conductivity | ASTMC177 | 0.20 | W/m/K | |
Vicat softening temperature | ASTMD15255 | 154 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Arc resistance 6 | ASTMD495 | PLC7 | ||
Hot wire ignition | HWI | UL746 | PLC1 | |
High arc combustion index | HAI | UL746 | PLC1 | |
High voltage arc tracing rate | HVTR | UL746 | PLC3 | |
Dissipation factor | 50Hz | ASTMD150 | 8E-04 | |
60Hz | ASTMD150 | 8E-04 | ||
1MHz | ASTMD150 | 7.5E-03 | ||
Dielectric constant | 1MHz | ASTMD150 | 3.05 | |
50Hz | ASTMD150 | 3.10 | ||
60Hz | ASTMD150 | 3.10 | ||
Volume resistivity | ASTMD257 | >1.0E+17 | ohms·cm | |
Dielectric strength | 3.20mm,inAir | ASTMD149 | 18 | KV/mm |
Compared to the anti leakage trace index | CTI | UL746 | PLC4 |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile impact strength 4 | ASTMD1822 | 158 | kJ/m² | |
Falling hammer impact | 23°C | ASTMD3029 | 102 | J |
hardness | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Rockwell hardness | M-Sale | ASTMD785 | 85 | |
R-Sale | ASTMD785 | 124 |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Extreme Oxygen Index | ASTMD2863 | 36 | % | |
UL flame retardant rating | 1.5mm | UL94 | V-0 | |
3.0mm | UL94 | 5VA |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.