PC LEXAN™ 4701R SABIC INNOVATIVE US
113
- Unit Price:
- $5477 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 62.3MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High temperature resistan transparent
- Application Areas:Electronic and electrical
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:3.20mm | 内部方法 | 0.80to1.0 | % |
Water absorption rate | 24hr | ASTMD570 | 0.19 | % |
Melt mass flow rate | 300°C/1.2kg | ASTMD1238 | 2.0 | g/10min |
300°C/6.1kg | ASTMD1238 | 9.0 | g/10min | |
Specific volume | ASTMD792 | 0.830 | cm³/g | |
density | ASTMD792 | 1.19 | g/cm³ |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile strength | 屈服 | ASTMD638 | 65.5 | Mpa |
断裂 | ASTMD638 | 77.9 | Mpa | |
elongation | 断裂 | ASTMD638 | 78 | % |
Bending modulus | 50.0mm跨距 | ASTMD790 | 2330 | Mpa |
bending strength | 屈服,50.0mm跨距 | ASTMD790 | 97.2 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 1.8MPa,未退火,3.20mm | ASTMD648 | 149 | °C |
RTIElec | UL746 | 130 | °C | |
Evolution Calendar intelligent importer | UL746 | 130 | °C | |
RTIStr | UL746 | 130 | °C | |
Linear coefficient of thermal expansion | MD:-40到95°C | ASTME831 | 8.1E-05 | cm/cm/°C |
specific heat | ASTMC351 | 1260 | J/kg/°C | |
thermal conductivity | ASTMC177 | 0.21 | W/m/K |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Dielectric strength | 3.20mm,inAir | ASTMD149 | 20 | KV/mm |
Volume resistivity | ASTMD257 | >2.5E+17 | ohms·cm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile impact strength | ASTMD1822 | 578 | kJ/m² | |
Falling hammer impact | 23°C | ASTMD3029 | 149 | J |
Impact strength of cantilever beam gap | 23°C | ASTMD256 | 370 | J/m |
23°C | ASTMD4812 | 3200 | J/m |
optical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
transmissivity | 2540µm | ASTMD1003 | 85.0 | % |
Haze | 2540µm | ASTMD1003 | 1.0 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.