Need Help? Contact Us service@plas.com
Get App

POM LNP™ LUBRICOMP™  KL-004AXD BK SABIC INNOVATIVE US

111
  • Unit Price:
    $3537 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    20MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:wear resistant
  • Application Areas:Electrical applications Electronic display Lighting applications
  • Color:--
  • Grade:--

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9552.0to2.5%
Shrinkage rateTD:24hrASTMD9552.0to2.5%
Shrinkage rateTD:24hrISO294-42.0to2.5%
Shrinkage rateMD:24hrISO294-42.0to2.5%
Water absorption rate24hr,50%RHASTMD5700.15%
Water absorption rateEquilibrium,23°C,50%RHISO620.26%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus 2ASTMD6382140Mpa
Tensile modulusISO527-2/12400Mpa
Tensile strengthYieldASTMD63851.1Mpa
Tensile stressYieldISO527-247.3Mpa
Tensile strengthBreakASTMD63850.9Mpa
Tensile stressBreakISO527-246.5Mpa
elongationYieldASTMD63811%
Tensile strainYieldISO527-210%
elongationBreakASTMD63818%
Tensile strainBreakISO527-223%
Bending modulusASTMD7902070Mpa
Bending modulusISO1782600Mpa
bending strength ASTMD79075.8Mpa
Bending stressISO17879.3Mpa
friction coefficientDynamicASTMD3702Modified0.29
friction coefficientStaticASTMD3702Modified0.15
Wear factor - WasherASTMD3702Modified15.010^-10in^5-min/ft-lb-hr
Thermal performanceTest ConditionTest MethodTest ResultUnit
Linear coefficient of thermal expansionTD:-40to40°CASTME8311.1E-04cm/cm/°C
Linear coefficient of thermal expansionTD:-40to40°CISO11359-21.1E-04cm/cm/°C
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTMD648157°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD64899.4°C
Hot deformation temperature 41.8MPa,Unannealed,64.0mmSpanISO75-2/Af98.0°C
Linear coefficient of thermal expansionMD:-40to40°CASTME8311.1E-04cm/cm/°C
Linear coefficient of thermal expansionMD:-40to40°CISO11359-21.1E-04cm/cm/°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Suspended wall beam gap impact strength 323°CISO180/1A4.0kJ/m²
UnnotchedIzodImpactStrength323°CISO180/1U45kJ/m²
Dart impact equipped with measuring instruments23°C,EnergyatPeakLoadASTMD37636.40J
Multi axis Instrumented Impact EnergyISO6603-20.770J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.