POM LNP™ STAT-KON™ KC-1004 SABIC INNOVATIVE US
101
- Unit Price:
- $9290 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 40MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:heat-resisting high strength Glass fiber reinforced
- Application Areas:Automotive Applications
- Color:--
- Grade:Injection grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Vertical flow direction: 24 hours | ISO294-4 | 1.7 | % | |
Flow direction: 24 hours | ISO294-4 | 0.69 | % | |
Water absorption rate | 24hr,50%RH | ASTMD570 | 0.20 | % |
Flow: 24 hours | ASTMD955 | 0.60到0.80 | % | |
Lateral flow: 24 hours | ASTMD955 | 1.6到1.8 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
--1 | ASTMD638 | 14500 | Mpa | |
yield | ASTMD638 | 121 | Mpa | |
ISO527-2 | 110 | Mpa | ||
crack | ASTMD638 | 121 | Mpa | |
ISO527-2 | 110 | Mpa | ||
yield | ASTMD638 | 1.6 | % | |
ISO527-2 | 1.4 | % | ||
crack | ASTMD638 | 1.6 | % | |
ISO527-2 | 1.4 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
0.45MPa, unannealed, 3.20mm | ASTMD648 | 162 | °C | |
0.45MPa, unannealed, 64.0mm span 4 | ISO75-2/Bf | 163 | °C | |
1.8MPa, unannealed, 3.20mm | ASTMD648 | 160 | °C | |
1.8MPa, unannealed, 64.0mm span 5 | ISO75-2/Af | 160 | °C | |
Flow: -40 to 40 ° C | ASTME831 | 6.8E-05 | cm/cm/°C | |
ISO11359-2 | 6.9E-05 | cm/cm/°C | ||
Horizontal: -40 to 40 ° C | ASTME831,ISO11359-2 | 3.1E-05 | cm/cm/°C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | ASTMD257 | 1.0E+2到1.0E+6 | ohms |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
23°C | ASTMD256 | 48 | J/m | |
23°C2 | ISO180/1A | 5.0 | kJ/m² | |
23°C | ASTMD4812 | 430 | J/m | |
23°C3 | ISO180/1U | 26 | kJ/m² | |
23°C,EnergyatPeakLoad | ASTMD3763 | 10.9 | J | |
-- | ISO6603-2 | 2.50 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.