PMMA ACRYPET™ MD001 MITUBISHI RAYON JAPAN
140
- Unit Price:
- $3502 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 24.1MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:Flame retardant High temperature resistan UV resistance
- Application Areas:Automotive components Lighting fixtures
- Color:--
- Grade:Heat resistant grade
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Refractive index | ASTM D-542 | 1.49 | ||
Full light transmission system | 2mm | ASTM D-1003 | 93 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
tensile strength | ASTM D-638 | 69[700] | MPa[KG/cm | |
Izod impact strength | 1/4槽口副 | ASTM D-256 | 16[1.6] | J/m[kg.cm/cm] |
Flexural strength | 1/4"棒 | ASTM D-790 | 103[1050] | MPa[KG/cm |
Flexural modulus of elasticity | 1/4"棒 | ASTM D-790 | 3.0[3.1×10 | GPa[KG/cm |
Rockwell hardness | ASTM D-785 | 92 | M Scale | |
Extension rate | ASTM D-638 | 7 | % |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
specific heat | JIS K-7123 | 1.5[0.35] | J/g.c[(cal/g/℃)] | |
Load deflection temperature | 1.82MPa | ASTM D-648 | 89 | °C |
Coefficient of thermal expansion | ASTM D-177 | 0.2 | W/m℃ | |
Spiral flow | 230℃ | MRC | 190-290 | mm |
Coefficient of linear expansion | ASTM D-696 | 6×10 | 1/℃ | |
Vicat softening temperature | 9.8N | ASTM D-1525 | 104 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Volume resistivity | JIS K-6911 | >10 | m[cm] | |
Surface resistivity | JIS K-6911 | >10 | ||
Arc resistance | JIS K-6911 | 没有痕迹 | ||
Insulation breakdown strength | 20[20] | MV/m[KV/mm] | ||
Dielectric loss tangent | 60Hz | 0.05 | ||
Dielectric constant | 60Hz | 3.7 |
Processing performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | ASTM D-955 | 0.2-0.5 | % |
Basic performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Water absorption rate | 24hr | ASTM D-570 | 0.3 | % |
Melt index | 230℃,37.3n | ASTM D-1238 | 6.0 | g/10min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.