Need Help? Contact Us service@plas.com
Get App

PA66 LNP™ LUBRILOY™  RF206-BK1B605 SABIC INNOVATIVE US

120
  • Unit Price:
    $3505 USD/MT
  • Packaging Specification:
    25 KG/PKG
  • Supply Quantity:
    10MT
  • Delivery Terms:
    FOB
  • Port of Loading:
    China Main Port
  • Accepted Payment Methods:
    T/T
  • Shipping:
    Negotiate supplier for shipping details

Supplier Information

ASIA PLASTIC EXCHANGE LIMITED

+86 755 2787 3515View
serv********View

For more detailed information including pricing, customization, and shipping, please contact supplier.

Material Description
Technical Data Sheet

Material Description

  • Material Properties:UV resistance Thermal stability
  • Application Areas:Textile application Home appliance components
  • Color:--
  • Grade:--

Technical Data Sheet Compare

physical property Test ConditionTest MethodTest ResultUnit
Shrinkage rateMD:24hrASTMD9550.60%
Shrinkage rateTD:24hrASTMD9551.2%
Water absorption rate24hr,50%RHASTMD5700.38%
Water absorption rateEquilibrium,23°C,50%RHISO620.66%
Mechanical performanceTest ConditionTest MethodTest ResultUnit
Tensile modulus 2ASTMD6388770Mpa
friction coefficientStaticASTMD3702Modified0.40
Wear factor - WasherASTMD3702Modified45.010^-10in^5-min/ft-lb-hr
Tensile modulusISO527-2/18470Mpa
Tensile strength 3BreakASTMD638121Mpa
Tensile stressBreakISO527-2/5118Mpa
Elongation rate 4BreakASTMD6382.5%
Tensile strainBreakISO527-2/52.3%
Bending modulus 450.0mmSpanASTMD7907060Mpa
Bending modulus 5ISO1787200Mpa
Bending stressISO178167Mpa
Bending strength 5Break,50.0mmSpanASTMD790173Mpa
friction coefficientDynamicASTMD3702Modified0.40
Thermal performanceTest ConditionTest MethodTest ResultUnit
Hot deformation temperature0.45MPa,Unannealed,3.20mmASTMD648258°C
Hot deformation temperature 70.45MPa,Unannealed,64.0mmSpanISO75-2/Bf252°C
Hot deformation temperature1.8MPa,Unannealed,3.20mmASTMD648241°C
Hot deformation temperature 71.8MPa,Unannealed,64.0mmSpanISO75-2/Af224°C
Linear coefficient of thermal expansionMD:-30to30°CASTMD6963.8E-05cm/cm/°C
Linear coefficient of thermal expansionTD:-30to30°CASTMD6967.5E-05cm/cm/°C
Impact performanceTest ConditionTest MethodTest ResultUnit
Suspended wall beam notch impact strength 623°CISO180/1A9.1kJ/m²
Unscented Izod Impact Strength 523°CISO180/1U35kJ/m²
Dart impact equipped with measuring instruments23°C,TotalEnergyASTMD376313.3J
Multi axis Instrumented Impact EnergyISO6603-23.70J
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.