PA66 LNP™ LUBRICOMP™ RFL4036 WT9-529 SABIC INNOVATIVE US
88
- Unit Price:
- $3536 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 20MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:High mobility Low friction coefficient Thermal stability Filler: Glass fiber reinf 30% filler by weight
- Application Areas:Electrical appliances Automotive sector sporting goods Lighting applications
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Shrinkage rate | MD:24hr | ASTMD955 | 0.40to0.60 | % |
TD:24hr | ASTMD955 | 1.0to3.0 | % | |
Water absorption rate | 24hr,50%RH | ASTMD570 | 0.37 | % |
Equilibrium,23°C,50%RH | ISO62 | 0.58 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile stress | Yield | ISO527-2/5 | 168 | Mpa |
Break | ISO527-2/5 | 158 | Mpa | |
Tensile strain | Yield | ISO527-2/5 | 2.8 | % |
Break | ISO527-2/5 | 2.8 | % | |
Bending stress | ISO178 | 219 | Mpa | |
friction coefficient | Dynamic | ASTMD3702Modified | 0.67 | |
Static | ASTMD3702Modified | 0.61 | ||
Elongation rate 3 | Yield | ASTMD638 | 2.8 | % |
Wear factor | Ring | ASTMD3702Modified | 0.250 | 10^-10in^5-min/ft-lb-hr |
Washer | ASTMD3702Modified | 5.00 | 10^-10in^5-min/ft-lb-hr | |
Tensile modulus 2 | ASTMD638 | 11700 | Mpa | |
Tensile strength 3 | Break | ASTMD638 | 160 | Mpa |
Yield | ASTMD638 | 160 | Mpa | |
Bending modulus 4 | 50.0mmSpan | ASTMD790 | 9260 | Mpa |
Bending strength 4 | Yield,50.0mmSpan | ASTMD790 | 233 | Mpa |
Tensile modulus | ISO527-2/1 | 10400 | Mpa | |
Elongation rate 4 | Break | ASTMD638 | 2.8 | % |
Bending modulus 5 | ISO178 | 8890 | Mpa | |
Bending strength 5 | Break,50.0mmSpan | ASTMD790 | 233 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature 7 | 1.8MPa,Unannealed,64.0mmSpan | ISO75-2/Af | 244 | °C |
0.45MPa,Unannealed,64.0mmSpan | ISO75-2/Bf | 258 | °C | |
Hot deformation temperature | 0.45MPa,Unannealed,3.20mm | ASTMD648 | 260 | °C |
1.8MPa,Unannealed,3.20mm | ASTMD648 | 249 | °C |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Suspended wall beam notch impact strength 6 | 23°C | ISO180/1A | 7.5 | kJ/m² |
Unscented Izod Impact Strength 5 | 23°C | ISO180/1U | 55 | kJ/m² |
Dart impact equipped with measuring instruments | 23°C,TotalEnergy | ASTMD3763 | 8.50 | J |
Multi axis Instrumented Impact Energy | ISO6603-2 | 2.50 | J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.