PA66 AKROMID® A3 1 S3 AKRO-PLASTIC GERMANY
203
- Unit Price:
- $3475 USD/MT
- Packaging Specification:
- 25 KG/PKG
- Supply Quantity:
- 43MT
- Delivery Terms:
- FOB
- Port of Loading:
- China Main Port
- Accepted Payment Methods:
- T/T
- Shipping:
- Negotiate supplier for shipping details
Supplier Information
ASIA PLASTIC EXCHANGE LIMITED
+86 755 2787 3515View
serv********View
For more detailed information including pricing, customization, and shipping, please contact supplier.
Material Description
Technical Data Sheet
Material Description
- Material Properties:enhance Thermal stability
- Application Areas:Industrial applications Automotive sector
- Color:--
- Grade:--
Technical Data Sheet
physical property | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
density | 23°C | ISO1183 | 1.10 | g/cm³ |
SpiralFlow | 内部方法 | 80.0 | CM | |
Shrinkage rate | TD | ISO294-4 | 2.2 | % |
MD | ISO294-4 | 2.1 | % | |
Humidity Absorption | 70°C | ISO1110 | 2.1 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Tensile modulus | ISO527-2/1 | 2700 | Mpa | |
Tensile stress | 屈服 | ISO527-2/50 | 63.0 | Mpa |
Bending stress | ISO178 | 90.0 | Mpa | |
Fracture bending strain | ISO178 | 7.5 | % | |
Tensile strain | 断裂 | ISO527-2/50 | >35 | % |
Bending modulus | ISO178 | 2500 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Hot deformation temperature | 0.45MPa,未退火 | ISO75-2/B | 213 | °C |
1.8MPa,未退火 | ISO75-2/A | 70.0 | °C | |
Melting temperature | DINEN11357-1 | 262 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Surface resistivity | IEC60093 | 1E+14 | ohms | |
Volume resistivity | IEC60093 | 1E+15 | ohms·cm | |
Leakage Trace Index | 解决方案A | IEC60112 | 600 | V |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Impact strength of cantilever beam gap | -40°C | ISO180/1A | 12 | kJ/m² |
-20°C | ISO180/1A | 12 | kJ/m² | |
23°C | ISO180/1A | 15 | kJ/m² | |
Charpy Notched Impact Strength | -30°C | ISO179/1eA | 10 | kJ/m² |
23°C | ISO179/1eA | 17 | kJ/m² |
flammability | Test Condition | Test Method | Test Result | Unit |
---|---|---|---|---|
Burning rate | 1.00mm | FMVSS302 | <100 | mm/min |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.