physical property | Test Condition | Test Method | Test Result | Unit |
---|
Shrinkage rate | TD | ISO294-4 | 1.4 | % |
Shrinkage rate | MD | ISO294-4 | 0.40 | % |
Water absorption rate | Saturation,23°C | ISO62 | 6.7to7.3 | % |
SpiralFlow2.3 | | 内部方法 | 99.0 | CM |
HumidityAbsorption-62%RH | 70°C | ISO1110 | 2.5to2.7 | % |
Mechanical performance | Test Condition | Test Method | Test Result | Unit |
---|
Bending stress 4 | | ISO178 | 200 | Mpa |
Bending modulus 4 | | ISO178 | 6100 | Mpa |
Tensile stress | Break | ISO527-2/5 | 140 | Mpa |
Tensile strain | Break | ISO527-2/5 | 3.5 | % |
Tensile modulus | | ISO527-2/1 | 6400 | Mpa |
Thermal performance | Test Condition | Test Method | Test Result | Unit |
---|
Hot deformation temperature | 0.45MPa,Unannealed | ISO75-2/B | 260 | °C |
Hot deformation temperature | 1.8MPa,Unannealed | ISO75-2/A | 245 | °C |
Melting temperature 5 | | DINEN11357-1 | 262 | °C |
Linear coefficient of thermal expansion | MD:23to80°C | ISO11359-2 | 3.4E-05 | cm/cm/°C |
Linear coefficient of thermal expansion | TD:23to80°C | ISO11359-2 | 1.1E-04 | cm/cm/°C |
TemperatureIndex | 50%LossofTensileStrength,5000hr | IEC216 | 160to175 | °C |
TemperatureIndex | 50%LossofTensileStrength,20000hr | IEC216 | 130to150 | °C |
Electrical performance | Test Condition | Test Method | Test Result | Unit |
---|
Leakage Trace Index | SolutionA | IEC60112 | 600 | V |
Surface resistivity | | IEC60093 | 1E+12 | ohms |
Volume resistivity | | IEC60093 | 1E+13 | ohms·cm |
Impact performance | Test Condition | Test Method | Test Result | Unit |
---|
Impact strength of simply supported beam without notch | -30°C | ISO179/1eU | 43 | kJ/m² |
Impact strength of simply supported beam without notch | 23°C | ISO179/1eU | 45 | kJ/m² |
hardness | Test Condition | Test Method | Test Result | Unit |
---|
Ball pressure hardness | H961/30 | ISO2039-1 | 200 | Mpa |
flammability | Test Condition | Test Method | Test Result | Unit |
---|
UL flame retardant rating | 0.8mm | UL94 | HB | |
Burning rate 6 | 1.00mm | FMVSS302 | <100 | mm/min |
GlowWireFlammability Index | 1.6mm | IEC60695-2-12 | 650 | °C |
Supplementary Information | Test Condition | Test Method | Test Result | Unit |
---|
ReinforcementContent | | ISO1172 | 15 | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.